Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 221 MPa | 32000 psi | IPC TM-650 2.4.18.3 |
Arlon 37N Polyimide Low-Flow 37N is a polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow is requir.. |
|||
Tensile Strength | 221 MPa | 32000 psi | IPC TM-650 2.4.18.3 |
Arlon 38N High Performance Polyimide Low-Flow 38N is an improved polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow.. |