Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 2.00 MPa | 290 psi | Estimated value; ISO 37 |
Kraton® D0243 E (SBS) Diblock Copolymer Description: Kraton D0243 E polymer is a clear, diblock copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Europe in the physical form identified:Kraton D02.. |
|||
Tensile Strength | 2.00 MPa | 290 psi | ISO 37 |
Kraton® D1118 E (SBS) Diblock Copolymer Description: Kraton D1118 E is a clear, diblock copolymer based on styrene and butadiene with a polystyrene content of 33%. It is supplied from Europe in the physical form identified: D1118 ET - sup.. |
|||
Tensile Strength | 2.00 MPa | 290 psi | |
Shin-Etsu Silicones KE-3418 Silicone, RTV Adhesive Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength | 2.00 MPa | 290 psi | |
Shin-Etsu Silicones KE-348 Silicone, RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength | 2.00 MPa | 290 psi | |
Shin-Etsu Silicones KE-44 Silicone, RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength | 2.00 MPa | 290 psi | |
Shin-Etsu Silicones KE-445 Silicone, RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength | 2.00 MPa | 290 psi | |
Shin-Etsu Silicones KE-1223 Silicone, Potting/Encapsulation RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength | 2.00 MPa | 290 psi | |
Shin-Etsu Silicones KE-45 Silicone, RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength | 2.00 MPa @Strain 20.0 % |
290 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan B 80 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 2.00 MPa @Strain 100 % |
290 psi @Strain 100 % |
ISO 37 |
BASF Elastollan C 65 A HPM TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tensile Strength | 2.00 MPa @Strain 20.0 % |
290 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan C 75 A HPM TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tensile Strength | 2.00 MPa | 290 psi | 20; ISO 37 |
BASF Elastollan SP 883 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tensile Strength | 2.00 MPa | 290 psi | average; in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® R82.80 High Performance Structural Foam AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver.. |
|||
Tensile Strength | >= 2.00 MPa | >= 290 psi | perpendicular to plane; ASTM C297 |
3A Composites Core Materials AIREX® T92.130 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,.. |
|||
Tensile Strength | 2.00 MPa @Strain 20.0 % |
290 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan B 85 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 2.00 MPa @Strain 20.0 % |
290 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan S 80 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 2.00 MPa @Strain 20.0 % |
290 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan S 85 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 2.00 MPa | 290 psi | average; in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® C70.75 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |