Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 19.0 MPa | 2760 psi | ASTM D412 |
S&E Specialty Polymers TufFlex™ GA-5330D PVC/PU Compound Application: 105°C, matte finish, flame retardant PVC/PU jacketing material designed for retractile cord applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 19.0 MPa | 2760 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® PP 1398 Conductive Thermoplastic Compound PRE-ELEC® PP 1398 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Tensile Strength | 19.0 MPa @Thickness 0.0500 mm |
2760 psi @Thickness 0.00197 in |
ASTM D882-02 |
NeXolve Essar™ Stretch 255 Polyimide High temperature colorless elastic polyimide. NeXolve Essar™ Stretch 255 combines polyimide high temperature survivability and stability with elastomer elasticity and optical clarity into a single .. |
|||
Tensile Strength | 19.0 MPa | 2760 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP TIVAR® 1000 PE-UHMW, virgin (ISO Data) TIVAR 1000 exhibits a very well balanced property profile. It combines a very good wear and abrasion resistance with an outstanding impact strength, even at temperatures below -200°C. |
|||
Tensile Strength | 19.0 MPa | 2760 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP TIVAR® Cleanstat PE-UHMW + specific additives (ISO Data) TIVAR CleanStat is a PE-UHMW grade for use in food processing and pharmaceutical industries. It exhibits static dissipative properties and has a food contact compliant composition. Very good wear an.. |
|||
Tensile Strength | 19.0 MPa | 2760 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP TIVAR® DS PE-UHMW + additives (ISO Data) TIVAR DS is a modified PE-UHMW with extremely high molecular weight. The latter in combination with a particular manufacturing process result in a PE-UHMW grade with superior wear and abrasion resis.. |
|||
Tensile Strength | 19.0 MPa | 2760 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP TIVAR® H.O.T. PE-UHMW + specific additives (ISO Data) TIVAR H.O.T. [Higher Operating Temperature] is formulated to maintain inherent PE-UHMW key properties over an extended service temperature range, in this way considerably increasing part life in low.. |
|||
Tensile Strength | 19.0 MPa | 2760 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP TIVAR® MD PE-UHMW + metal detectable additive (ISO Data) This PE-UHMW grade with extremely high degree of polymerisation contains a metal detectable additive which does hardly affect the inherent PE-UHMW key properties. TIVAR MD presents excellent toughne.. |
|||
Tensile Strength | 19.0 MPa | 2760 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP TIVAR® TECH PE-UHMW + MoS2 (ISO Data) This PE-UHMW grade with extremely high degree of polymerisation contains molybdenum disulphide, resulting in a material with improved wear resistance and sliding properties over TIVAR 1000. |
|||
Tensile Strength | 19.0 MPa | 2760 psi | ISO 37 |
Termopol Termoton® V2GA1050d TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
Tensile Strength | 19.0 MPa | 2760 psi | |
Sawbones Solid Rigid Polyurethane Foam 40 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |
|||
Tensile Strength | 19.0 MPa @Strain 100 % |
2760 psi @Strain 100 % |
ISO 37 |
BASF Elastollan 1154 D FHF TPUR Flame Retardant Halogen Free Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tensile Strength | 19.0 MPa @Strain 100 % |
2760 psi @Strain 100 % |
ISO 37 |
BASF Elastollan B 64 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 19.0 MPa | 2760 psi | ISO 37 |
Termopol Termoton® K2GA4055D TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |