Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 9.31 MPa | 1350 psi | ASTM D638 |
S&E Specialty Polymers GM-3255 PVC Application: Non-toxic PVC material designed for molding applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 9.31 MPa | 1350 psi | ASTM D412 |
Kraton® G2806 GO-N (SEBS) Compound Description: Kraton G2806 GO-N is a compound designed for film applications in the Personal Care market: Kraton G2806 GO-N - supplied as an organic dusted dense pelletRegion: Asia Pacific, Europe, J.. |
|||
Tensile Strength | >= 9.32 MPa | >= 1350 psi | ASTM D 638 |
Karina 700D40/356-AT Green PVC Compound Non toxic PVC compound, recommended for injection of inhalation maskInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 9.30 MPa | 1350 psi | |
Momentive Performance Materials TUFELâ„¢ II 94305 Low Volatile Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 9.30 MPa | 1350 psi | |
Momentive Performance Materials TUFELâ„¢ II 94306 Low Volatile Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 9.30 MPa | 1350 psi | |
Momentive Performance Materials FSE7570-D1 Heat Cured Fluorosilicone Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 9.30 MPa | 1350 psi | |
Shin-Etsu Silicones LIMSâ„¢ KE1950-50A/B Elastomer KE-1950-50 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |
|||
Tensile Strength | 9.31 MPa | 1350 psi | Silicone Property; ASTM D412 |
Arlon 10502R020 0.020" (0.508 mm) Cured Silicone Rubber (Unsupported) Design/Construction:Material: Cured Silicone RubberLiner: Polyethylene Recommended Cure Cycle: Product delivered curedRecommended Post Cure Cycle: Product delivered post-curedAppearance: Red silicon.. |
|||
Tensile Strength | 9.30 MPa | 1350 psi | ISO 37 |
AlphaGary Evoprene™ 032 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Tensile Strength | 9.31 MPa | 1350 psi | |
AlphaGary Garaflex™ E X 05-384-G LCF Vinyl Thermoplastic Elastomer Garaflex™ E is a vinyl based thermoplastic elastomer used mostly in wire and cable60°C rated flexible compound for microphone & audio applications |
|||
Tensile Strength | 9.31 MPa | 1350 psi | Silicone Property; ASTM D412 |
Arlon R30342R032 0.032" (0.813 mm) Cured Silicone Rubber Design/Construction:Product: Cured Silicone Rubber Liner: PolyethyleneAppearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used to w.. |