Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Addisilâ„¢ 1080 E Industrial Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ CLS 8150 Liquid Silicone Rubber - Self-Bonding / Customized This LSR elastomer is a self-bonding, customized, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ FFSL 7286/40 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2030 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2630 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2730 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3486/20 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3486/50 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3596/30 Liquid Silicone Rubber - Self-Lubricating / Ultra Low Compression Set This LSR elastomer is a self-lubricating, ultra low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycl.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3785/30 Liquid Silicone Rubber - Self-Lubricating / Standard This LSR elastomer is a self-lubricating, standard, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at eleva.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials HV 6/600 Heat Cured Rubber - STEAM Resistant Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3386/40 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tensile Strength | >= 8.00 MPa | >= 1160 psi | ASTM F152 |
Thermoseal RG-S160 PTG Gasketing Thermoseal RG-S160 offers exceptional sealability and crush resistance in a wide range of applications. RG-S160 is composed of a blend of aramid, mineral, and cellulose fibers and graphite and other.. |
|||
Tensile Strength | 8.00 MPa @Strain 300 % |
1160 psi @Strain 300 % |
ISO 37 |
BASF Elastollan 1185 A W TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tensile Strength | 8.00 MPa @Strain 300 % |
1160 psi @Strain 300 % |
ISO 37 |
BASF Elastollan S 80 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 8.00 MPa @Strain 300 % |
1160 psi @Strain 300 % |
ISO 37 |
BASF Elastollan S 85 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 8.00 MPa @Strain 20.0 % |
1160 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan S 95 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | ASTM D412 |
Dynasol Solprene® 9618 Multi-branched Thermoplastic Rubber (Multi-branched SBS) Solprene 9618 is a 69/31 Butadiene-Styrene multi arm copolymer, polymerized in solution process. It is stabilized with non-staining antioxidant system. This product is presented as a free flowing po.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | fill; ISO 37 Type 2 |
Rogers Corporation Bisco® A2 R 3.0 Engineered Solid Silicone Mass Layer, Fiberglass Reinforced Sound Barrier BISCO® A2 Fiberglass Reinforced Sound Barrier provides a similar level of sound absorption and flame resistance as the non-reinforced A2 Sound Barrier with the addition of increased tensile and tea.. |
|||
Tensile Strength | 8.00 MPa | 1160 psi | Flatwise |
Henkel Hysol EA 9257 Primer Waterborne, corrosion-inhibiting primer, maintains surface bondability after multiple prebonding cure cycles. Meets SCAQMD Rule 1124. Replacement for Hysol EA 9210B.Applications: Sprayable Low Visc.. |
|||
Tensile Strength | 8.00 MPa @Strain 20.0 % |
1160 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan 695 AU TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |