Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 79.3 MPa | 11500 psi | ASTM D638 |
Quadrant EPP Nylatron® MD PA6, Metal-detectable Nylon (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products Broadest size range availability Good mechanical and electrical properties Ideal balance of strength and toughness Cast as finished parts and n.. |
|||
Tensile Strength | 79.3 MPa | 11500 psi | ASTM D638 |
Quadrant EPP Semitron® MP-370 (ASTM Product Data Sheet) |
|||
Tensile Strength | 79.3 MPa | 11500 psi | ASTM D638 |
Quantum PET Information provided by Quantum Advanced Engineering Plastics |
|||
Tensile Strength | 79.3 MPa | 11500 psi | ASTM D638 |
Teknor Apex Chemlon® 212 Nylon 6, Unreinforced Features: Lubricated, General Purpose; General purpose nylon 6; Slightly tougher and more ductile than nylon 66 Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex.. |
|||
Tensile Strength | 79.3 MPa | 11500 psi | ASTM D638 |
Ensinger Tecapeek® XP-95 Compression Molded PEEK Compound, 15% PTFE Filled Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Tensile Strength | 79.3 MPa | 11500 psi | ASTM D638 |
Quadrant EPP Semitron® ESd 420- CM Dissipative Polyetherimide(ASTM Product Data Sheet) |