Polymer Property : Tensile Strength = 41.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 41.0 MPa

@Thickness 0.0500 mm
5950 psi

@Thickness 0.00197 in
ASTM D882-02
NeXolve UV Blocking Optionox® Polyimide Film/Coating
Highly UV durable with excellent weatherability and stability to ozone.Optinox® films and coatings are highly UV durable and exhibit excellent weathering durability, including very high stability ..
Tensile Strength 41.0 MPa
5950 psi
ASTM D638
Kolon KOCETAL® TF304 Wear Modified Acetal Resin
PTFE powder added, improved wear property. Applications: High speed, high load and wear resistant products. Information provided by API-Kolon.
Tensile Strength 41.0 MPa
5950 psi
ASTM D412
GRECO ISOTHANE 1055DE Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are Poly(adipate)ester based thermoplastic polyurethanes with good balanced qualities. They exhibit good toughness, abrasive resistance, solvent resistance, and transp..
Tensile Strength 41.0 MPa
5950 psi
ASTM D412
GRECO ISOTHANE 3090AF Polyether TPU Resin
ISOTHANE 3000F Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These pro..
Tensile Strength 41.0 MPa
5950 psi
ASTM D412
GRECO ISOTHANE 5090A Polyether TPU Resin
ISOTHANE 5000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent bio-compatibility, hydrolytic resistance, fungus resistance, and low temperature performance pro..
Tensile Strength 41.0 MPa
5950 psi
ASTM D638
KYDEX® V103 High Impact Fire-Rated Thermoforming Sheet
Features:Formulated to substitute for FR-ABS sheetVery good impact resistanceEasy to form with excellent part definition and deep-draw characteristicsSuggested Applications:Equipment HousingsExhibit..
Tensile Strength 41.0 MPa
5950 psi
ASTM D412
GRECO ISOTHANE 1065D Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products ..
Tensile Strength 41.0 MPa
5950 psi
ASTM D412
GRECO ISOTHANE 1095A Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products ..
Tensile Strength 41.0 MPa
5950 psi
ASTM D412
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol
Tensile Strength 41.0 MPa
5950 psi
ASTM D412
Lubrizol ESTANE® 58137 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Tensile Strength 41.0 MPa
5950 psi
ASTM D882-80, Method A - 100%
DuPont™ Tedlar® SP TTR10AH9 Transparent Polyvinyl Fluoride Film
Transparent, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistanc..
Tensile Strength 41.0 MPa
5950 psi
ASTM D882-80, Method A - 100%
DuPont™ Tedlar® SP TUA10AH9 Polyvinyl Fluoride Film
UV Screening, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistan..
Tensile Strength 41.0 MPa
5950 psi
2 in/min; ASTM D638
Braskem F1000HC Homopolymer Polypropylene
Description: Very High Flexural ModulusApplications: Suggested Uses Include Compounding, Automotive, AppliancesThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177..
Tensile Strength 41.0 MPa
5950 psi
ASTM D412
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and Asia Information provided by Lubrizol.