Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 3.65 MPa @Strain 100 % |
529 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B70CA Polyvinyl Chloride, Flexible (PVC, Flexible) Improved adhesion.Information provided by PolyOne |
|||
Tensile Strength | 3.65 MPa @Strain 100 % |
529 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B70CB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 3.65 MPa | 530 psi | Side 1; ASTM D412 |
Arlon 19586R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 1523 Style FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the production mat.. |
|||
Tensile Strength | 3.65 MPa | 530 psi | Side 1, Silicone Property; ASTM D412 |
Arlon 51586R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Red silicone gum and rubber on fiberglass clot.. |
|||
Tensile Strength | 3.65 MPa | 530 psi | Side 1, Silicone Property; ASTM D412 |
Arlon 51586R015H 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production mat.. |
|||
Tensile Strength | 3.65 MPa | 530 psi | Side 1, Silicone Property; ASTM D412 |
Arlon 51586R052 0.052" (1.32 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothInterleave: Polyethylene.. |
|||
Tensile Strength | 3.65 MPa | 530 psi | Side 2, Layer 1, Silicone Property; ASTM D412 |
Arlon 51588R019 0.019" (0.483 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2, Layer 1: Cured Silicone RubberSide 2, Layer 2: Uncured Silicone Rubber Interleave: Polyethylene Appearanc.. |
|||
Tensile Strength | 3.65 MPa | 530 psi | Side 1 Silicone Property; ASTM D412 |
Arlon 55586XC028 0.0295" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Tensile Strength | 3.65 MPa | 530 psi | Side 1, Silicone Property; ASTM D412 |
Arlon 56586R026 0.027" (0.686 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Red silicone gum and rubber on fiberglass clo.. |
|||
Tensile Strength | 3.65 MPa | 530 psi | Side 1, Silicone Property; ASTM D412 |
Arlon 49586B010 0.0115" (0.292 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1681 FiberglassSide 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mater.. |
|||
Tensile Strength | 3.65 MPa | 530 psi | Layer 2, Silicone Property; ASTM D412 |
Arlon 55589G028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Green silicone gum and rubber on fiberglass Th.. |
|||
Tensile Strength | 3.65 MPa | 530 psi | Layer 2, Silicone Property; ASTM D412 |
Arlon 55589R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum and rubber on fiberglass This.. |