Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 27.0 MPa | 3920 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® PP 1392 Carbon Black Filled Conductive Thermoplastic Compound PRE-ELEC® PP 1392 is a carbon black filled conductive thermoplastic compound based on polypropylene. In addition to a low electrical resistivity PRE-ELEC® PP 1392 has an excellent balance of mecha.. |
|||
Tensile Strength | 27.0 MPa | 3920 psi | ISO 37 |
Kraton® D1184 A (SBS) Branched Block Copolymer Description: Kraton D1184 A is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows.. |
|||
Tensile Strength | 27.0 MPa | 3920 psi | ISO 37 |
Kraton® D1184 E (SBS) Branched Block Copolymer Description: Kraton D1184 E is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows.. |
|||
Tensile Strength | 27.0 MPa | 3920 psi | ISO 527 |
MRC Polymers MAXTEL™ 640-BK Polypropylene Copolymer • For extrusion or injection molding• Excellent process ability.Information provided by MRC Polymers Inc. |
|||
Tensile Strength | 27.0 MPa | 3920 psi | MD; ISO 527 |
Lucobit Lucofin® 1400HN Powder Ethylene Butyl Acrylate Lucofin 1400HN Powder is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN Powder is softer and more flexible than ethy.. |
|||
Tensile Strength | 27.0 MPa | 3920 psi | |
Sawbones Solid Rigid Polyurethane Foam 50 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |
|||
Tensile Strength | 27.0 - 35.0 MPa | 3920 - 5080 psi | ISO 527 |
BASF Ecovio® C2224 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2224 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |
|||
Tensile Strength | >= 27.0 MPa | >= 3920 psi | Grade A |
Shandong Dongyue Polymer DF-101 PTFE Molding Powder (Medium Particle Size) Usage: Can be processed to film, sheet, rob, gasket, axletree and presintered material.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE shou.. |