Mechanical Properties Metric English Comments
Tensile Strength 2.41 MPa
350 psi
ASTM D412
Parker Chomerics CHOFORM® 5513 Conductive Form-in-Place Gasket
Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material..
Tensile Strength >= 2.41 MPa
>= 350 psi
ASTM D412
Parker Chomerics CHO-FORM® 5518 Robotically Dispensed Gasketing
Description: CHO-FORM® 5518 Two-component, thermal cure silicone system with Ag/Cu particle filler. Minimum cure temperature is only 85°C (185°F). Formulated for painted, plated or metalized plas..
Tensile Strength 2.41 MPa

@Strain 100 %
350 psi

@Strain 100 %
ASTM D412
Vicone High Performance Rubber VicoSil™ 159DLK-RD High Performance Silicone Rubber
Meets AMS 3302 Silicone 50 Durometer.
Tensile Strength 2.41 MPa
350 psi
Side 2, Compound; ASTM D412
Arlon R36133N062 0.062" (1.57 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Layer 1: Cured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production ma..
Tensile Strength 2.41 MPa
350 psi
Typical properties of film cast from toluene solution; ASTM D412
Kraton® G1726 M (SEBS) Linear Triblock Copolymer
Description: Kraton G1726 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form ide..