Arlon R36133N062 0.062" (1.57 mm) Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R36133N062 0.062" (1.57 mm) Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Layer 1: Cured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
Side 1, Compound; Arlon SQA-TMS-024
Thickness 102 microns
4.00 mil
Side 1; Arlon SQA-TMS-003
457 microns
18.0 mil
Substrate; Arlon SQA-TMS-003
1020 microns
40.0 mil
Side 2; Arlon SQA-TMS-003
1570 microns
62.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 52
52
Side 1, Compound; ASTM D2240
92
92
Side 2, Compound; ASTM D2240
Tensile Strength 2.41 MPa
350 psi
Side 2, Compound; ASTM D412
6.14 MPa
890 psi
Side 1, Compound; ASTM D412
Elongation at Break 5.0 %
5.0 %
Side 2, Compound; ASTM D412
550 %
550 %
Side 1, Compound; ASTM D412
Toughness 7.00 J
5.16 ft-lb
Modified ASTM D412
2072 J
1528 ft-lb
Modified ASTM D412
Thermal Properties Metric English Comments
Specific Heat Capacity 0.320 J/g-°C
0.0765 BTU/lb-°F
ASTM E 1461-01
Thermal Conductivity 6.50 W/m-K
45.1 BTU-in/hr-ft²-°F
ASTM E 1530 & ASTM E 1461-01
Descriptive Properties Value Comments
Color Naturally Beige
Side 2
Red
Side 1