Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 17.2 MPa | >= 2490 psi | ASTM D412 |
S&E Specialty Polymers FS-1000K PVC Application: High Grade, RoHS compliant, lead-free, low smoke generating, highly flame retardant jacketing compound designed for Plenum cable application. Compound exhibits excellent processability.. |
|||
Tensile Strength | 17.2 MPa | 2490 psi | ASTM D638 |
S&E Specialty Polymers G-2184 Application: Clear, general purpose extrusion compound designed for profile extrusion applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 17.2 MPa | 2490 psi | ASTM D412 |
S&E Specialty Polymers GA-1057H1-VW1LF PVC Application: Lead free 105° C, flat ribbon cable insulation.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | >= 17.2 MPa | >= 2490 psi | ASTM D412 |
S&E Specialty Polymers TufShield™ FS-1000H-UVFG Insulating Compound Application: A UV and fungus resistant lead-free, low smoke generating, highly flame retardant jacketing and insulation compound designed for Plenum cable application. Compound exhibits excellent pr.. |
|||
Tensile Strength | 17.2 MPa | 2490 psi | ASTM D412 |
S&E Specialty Polymers TufTech™ G-2184M PVC Compound Application: A RoHS compliant, general purpose PVC based compound designed for molding applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 17.2 MPa | 2490 psi | ASTM D412 |
S&E Specialty Polymers TufTech™ GA-509-KHA PVC Compound Application: 105°C rated jacketing compound with good low temperature and aging properties.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 17.2 MPa | 2490 psi | ASTM D412 |
S&E Specialty Polymers TufTech™ GA-96-120 PVC Compound Application: A Flame Retardant Wire & Cable Jacketing Compound Rated at 75°C With Superior Low Temperature Properties and UV Resistance.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 17.2 MPa | 2490 psi | ASTM D412 |
S&E Specialty Polymers TufTech™ GA-8705-03 Natural PVC Compound Application: A 75°C, RoHS compliant, PVC based compound, suitable for Riser jacketing applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 17.2 MPa | 2490 psi | ASTM D412 |
S&E Specialty Polymers TufTech™ GM-93-060LT PVC Compound Application: A clear, non-toxic, extrusion compound for food contact use. Compound exhibits excellent low temperature flexibility.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | >= 17.2 MPa | >= 2490 psi | Measured on solution cast film from toluene; BAM 1245 |
Kraton® G1641 H (SEBS) Linear Triblock Copolymer Description: Kraton G1641 H is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 33%. It is supplied from North America in the physical form ide.. |
|||
Tensile Strength | >= 17.2 MPa | >= 2490 psi | ASTM D 638 |
Karina E 70/222-D-IS-SD Clear PVC Compound PVC compound recommended for rolled mill of notebook covering.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 17.2 MPa | 2500 psi | ASTM D638 |
Techmer ES HiFill® PP 0159 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Tensile Strength | 17.2 MPa | 2490 psi | ASTM D638 |
Saint-Gobain Rulon® 123 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Tensile Strength | 17.2 MPa | 2500 psi | |
AlphaGary Garaflex™ E 4777-A6 LCF Vinyl Thermoplastic Elastomer Garaflex™ E is a vinyl based thermoplastic elastomer used mostly in wire and cable105°C rated low gloss flexible cord jacket compound |
|||
Tensile Strength | 17.2 MPa | 2500 psi | |
AlphaGary GPE 2001-R Flame Retardant Polyethylene GPE 2001-R is a PBB, PBBE and PBBO free, flame Retardant thermoplastic insulation and spline compound intended for communications cable (90°C rated). |
|||
Tensile Strength | 17.2 MPa | 2500 psi | |
AlphaGary GW 3040 LCF Flame Retardant Polyvinyl Chloride 80°C rated jacket compound for riser application |
|||
Tensile Strength | 17.2 MPa | 2500 psi | |
AlphaGary Smokeguard™ LS III 1093 Low Smoke Polyvinyl Chloride 75°C Plenum Jacket |
|||
Tensile Strength | 17.2 MPa | 2500 psi | |
AlphaGary Smokeguard™ LS V 1116 Low Smoke Polyvinyl Chloride 75°C Plenum Jacket. Low Cost Plenum Jacket - Molybdenum Free |
|||
Tensile Strength | 17.2 MPa | 2500 psi | |
AlphaGary Smokeguard™ LS V 1118 Low Smoke Polyvinyl Chloride 75°C Plenum Jacket Low Cost Plenum Jacket - Molybdenum Free |
|||
Tensile Strength | 17.2 MPa | 2500 psi | |
AlphaGary GW 2462 H VW1 LCF Flame Retardant Polyvinyl Chloride 105°C rated semi-rigid insulation compound |
|||
Tensile Strength | 17.2 MPa | 2500 psi | |
AlphaGary GW 3035-VW1 LCF Flame Retardant Polyvinyl Chloride 60°C or 75°C rated flexible jacket compound for patch cord |
|||
Tensile Strength | 17.2 MPa | 2500 psi | |
AlphaGary Smokeguard™ HP 505 High Performance Fluoropolymer Smokeguard™ HP is a high performance fluoropolymer compound with excellent flame and smoke properties intended for difficult constructions and test requirements |
|||
Tensile Strength | 17.2 MPa | 2500 psi | |
AlphaGary Smokeguard™ LS III 1041 Low Smoke Polyvinyl Chloride Azoxymethane Free Low Cost Fiber Optic Jacket/Buffer Compound. Application example includes Optical Cables |
|||
Tensile Strength | 17.2 MPa | 2500 psi | |
AlphaGary Smokeguard™ LS III 1056 Low Smoke Polyvinyl Chloride 75°C Plenum Jacket |
|||
Tensile Strength | 17.2 MPa | 2500 psi | |
AlphaGary Smokeguard™ LS III 1057 Low Smoke Polyvinyl Chloride 75°C Plenum Jacket |
|||
Tensile Strength | 17.2 MPa | 2500 psi | |
AlphaGary Smokeguard™ LS III 1071 A Low Smoke Polyvinyl Chloride 75°C Plenum Jacket |
|||
Tensile Strength | 17.2 MPa | 2500 psi | |
AlphaGary Smokeguard™ LS III 1091 A1 Low Smoke Polyvinyl Chloride 60°C Plenum Jacket |
|||
Tensile Strength | 17.2 MPa | 2500 psi | |
AlphaGary Smokeguard™ LS III 1011 Low Smoke Polyvinyl Chloride 75°C Plenum Jacket |
|||
Tensile Strength | 17.2 MPa | 2500 psi | across grain; ASTM F152 |
Garlock BLUE-GARD® 3700 Compressed Aramid Fiber Gasketing, EPDM Binder Aramid fiber, high-temperature fillers, and EPDM binder. For service areas with weak causticsExcellent SealabilityUnique blend of aramid fibers, fillers, and a EPDM rubber binder provides improved t.. |