Mechanical Properties Metric English Comments
Tensile Strength 15.0 MPa
2180 psi
ASTM D412
Multibase TPSiV® 3111-70A Thermoplastic Elastomer
TPSiV™ material for injection molding and extrusion applicationsAPPLICATIONS: Solution for appliance, sports and leisure, and construction applications where excellent hydrolysis resistance, high a..
Tensile Strength >= 15.0 MPa
>= 2180 psi
Type IV, 500mm/min; ASTM D638
S&E Specialty Polymers XP23-566-1 PVC
Description: PVC weatherable, integral colored, filledApplication: Low gloss lift gate molding compound which meets Chrysler MSDC 543.Information provided by S&E Specialty Polymers
Tensile Strength >= 15.0 MPa
>= 2180 psi
Type IV, 500mm/min; ISO 37
S&E Specialty Polymers XP44-11 PVC
Description: PVC weatherable, integral colored, filledApplication: Body side skin extrusion and injection molding compound meets GMP.PVC.015, GMP.PVC.093, GMP.PVC.094, Chrysler MSDC 543, and Ford WS..
Tensile Strength >= 15.0 MPa
>= 2180 psi
DIN 53504
NEXA® PFX9014 Perfluoroelastomer
NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi..
Tensile Strength 15.0 MPa
2180 psi
at Yield; ISO 527-1/-2
Quadrant EPP Symalit® 1000 PFA unfilled, lining industries (ISO Data)
Symalit 1000 PFA is made from a fluoropolymer resin that is a copolymer of tetrafluoroethylene and perfluorovinylether. It exhibits good mechanical properties combined with excellent electrical prop..
Tensile Strength 15.0 MPa
2180 psi
ASTM D2095
Permabond UV649 UV-curable Adhesive
PERMABOND UV649 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon..
Tensile Strength >= 15.0 MPa
>= 2180 psi
Type IV, 500mm/min; ISO 37
S&E Specialty Polymers XP110-13-45 PVC
Description: PVC weatherable, integral colored, filledApplication: Body side end cap extrusion and injection molding compound designed for anti-stain which meets GMP.PVC.093, GMP.PVC.094 & Chrysler ..
Tensile Strength 15.0 - 20.0 MPa
2180 - 2900 psi
ASTM D4894
Isoflon PTFE + 50% Stainless Steel (AISI 316 L) Polytetrafluoroethylene with 50% INOX Stainless Steel
Properties:Improved compression resistance (very low cold flow)Low permeabilityApplications: Dynamic seals operating under high pressure and when chemical resistance is a necessity.Information prov..
Tensile Strength 15.0 - 20.0 MPa
2180 - 2900 psi
molded; ASTM D4745
Guarniflon PTFE G418 Polytetrafluoroethylene 15% Glass Fiber, 5% Molybdenum Disulfide
PTFE G Special Compound with glass fiber and molybdenum disulphiteInformation provided by Guarniflon®
Tensile Strength 15.0 - 20.0 MPa
2180 - 2900 psi
molded; ASTM D4894, ASTM D4745
Guarniflon PTFE G415 Polytetrafluoroethylene 25% Soft Carbon
PTFE G Standard Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high ..
Tensile Strength 15.0 - 35.0 MPa
2180 - 5080 psi
Moulding Direction; BS2782:Pt3
Dalau Dalcon 001 100% Virgin PTFE
Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi..
Tensile Strength 15.0 - 35.0 MPa
2180 - 5080 psi
Moulding Direction; BS2782:Pt3
Dalau Dalcon 001 100% Virgin PTFE
Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi..
Tensile Strength 15.0 MPa

@Strain 100 %
2180 psi

@Strain 100 %
ISO 37
BASF Elastollan 1198 A TPUR
Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi..
Tensile Strength 15.0 MPa

@Strain 300 %
2180 psi

@Strain 300 %
ISO 37
BASF Elastollan B 85 A TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup..
Tensile Strength 15.0 MPa
2180 psi
AlphaGary Megolon™ IN200 Low Smoke Halogen Free
General purpose insulation grade suitable for use up to 1KV. Application examples include Radio Frequency / Data Optical / Special Fire Survival.
Tensile Strength 15.0 MPa
2180 psi
AlphaGary Megolon™ S300 Low Smoke Halogen Free
General purpose sheathing compound with good mechanical and processing properties. Application examples include Data, Optical / Radio Frequency.
Tensile Strength 15.0 MPa
2180 psi
fill; ISO 37 Type 2
Rogers Corporation Bisco® A2 R 1.5 Engineered Solid Silicone Mass Layer, Fiberglass Reinforced Sound Barrier
BISCO® A2 Fiberglass Reinforced Sound Barrier provides a similar level of sound absorption and flame resistance as the non-reinforced A2 Sound Barrier with the addition of increased tensile and tea..
Tensile Strength 15.0 MPa

@Strain 20.0 %
2180 psi

@Strain 20.0 %
ISO 37
BASF Elastollan S 60 D TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
Tensile Strength 15.0 - 20.0 MPa
2180 - 2900 psi
molded; ASTM D4894, ASTM D4745
Guarniflon PTFE G412 Polytetrafluoroethylene 15% Graphite
PTFE G Standard Compound with graphite.Properties: Extremely low coefficient of friction. Fairly good compressive strength. Enhanced chemical resistance. Good wear resistance. Good thermal diss..
Tensile Strength >= 15.0 MPa
>= 2180 psi
extruded; ASTM D4894, ASTM D4745
Guarniflon PTFE G403 Polytetrafluoroethylene 15% Glass Fiber
PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re..