Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 2.00 mm |
0.018 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 100TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100TL NC010 is a high viscosity acetal homopolymer with 1.5% Teflon® PTFE Micropowder.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 2.00 mm |
0.018 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas.. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Time 86400 sec |
0.018 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12 LNP* LUBRICOMP* IL004 is a compound based on Nylon 6/12 resin containing 20% PTFE. Added features of this material include: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Time 86400 sec |
0.018 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12 (Asia Pacific) LNP* Lubricomp* IL004 is a compound based on Nylon 6/12 resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.020 cm/cm @Time 86400 sec |
0.018 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 (Asia Pacific) LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing Glass Bead. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.020 cm/cm @Time 86400 sec |
0.018 - 0.020 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 (Asia Pacific) LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing Glass Bead. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Time 86400 sec |
0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly LNP* STAT-LOY* K3000SZ is a compound based on Acetal Copolymer resin. Added feature of this material is: AntiSstatic. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Time 86400 sec |
0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly (Asia Pacific) LNP* Stat-loy* K3000SZ is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Time 86400 sec |
0.018 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-LOY K3000Z Acetal LNP* STAT-LOY* K3000Z is a compound based on unfilled Acetal resin. Added feature of this material is: Antistat. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.020 cm/cm @Time 86400 sec |
0.018 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing 40% Glass Bead. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.020 cm/cm @Time 86400 sec |
0.018 - 0.020 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing 40% Glass Bead. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 3.20 mm |
0.018 in/in @Thickness 0.126 in |
DAM |
DuPont Performance Polymers Zytel® ST811HS NC010 Nylon 6
(Unverified Data**) Zytel® ST811HS is a flexible, heat stabilized Super Tough polyamide 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores and fastene.. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 2.00 mm |
0.018 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® ST811HS NC010 Nylon 6
(Unverified Data**) Zytel® ST811HS is a flexible, heat stabilized Super Tough polyamide 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores and fastene.. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.021 cm/cm @Thickness 4.00 mm |
0.018 - 0.021 in/in @Thickness 0.157 in |
Parallel, 24h; ISO 294-4 |
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod.. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 2.00 mm |
0.018 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® FG100TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100TL is a high viscosity acetal homopolymer, containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.Inform.. |