Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.948 - 0.955 g/cc @Temperature 23.0 °C |
0.0342 - 0.0345 lb/in³ @Temperature 73.4 °F |
|
Kazanorgsintez PE2NT21-13 High Density Polyethylene Composite Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended for injection molding processin.. |
|||
Density | 0.948 - 0.955 g/cc @Temperature 23.0 °C |
0.0342 - 0.0345 lb/in³ @Temperature 73.4 °F |
|
Kazanorgsintez PE2NT26-13 High Density Polyethylene Composite Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended for injection molding processin.. |
|||
Density | 0.949 - 0.955 g/cc @Temperature 20.0 °C |
0.0343 - 0.0345 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez PE2NT74-15 High Density Polyethylene for Blow Molding Production Method: Gaseous-phase method. Application: Compositions are intended for goods produced by injection molding method.Information Provided by Kazanorgsintez |
|||
Density | 0.950 - 0.956 g/cc @Temperature 23.0 °C |
0.0343 - 0.0345 lb/in³ @Temperature 73.4 °F |
|
Kazanorgsintez PE2NT75-15 High Density Polyethylene for Blow Molding Production Method: Gaseous-phase method. Application: Compositions are intended for goods produced by injection molding method.Information Provided by Kazanorgsintez |