Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.15 g/cc @Temperature 25.0 °C |
0.0415 lb/in³ @Temperature 77.0 °F |
Solid |
3D Systems Accura® ClearVue™ Free (SL 7870) Stereolithography Plastic High clarity plastic for a multitude of applicationsFeaturesClear and transparentRigid and toughGreat for headlamps, bottles and transparent assembliesExcellent humidity/moisture resistanceAll infor.. |
|||
Density | 1.15 g/cc @Temperature 25.0 °C |
0.0415 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® SG-470 Rigid Polyol Description: Pluracol® SG-470 polyol is a clear, light colored, sucrose/glycerine polyol. Pluracol SG-450 contains no nitrogen. The high sucrose content with the high hydroxyl number has excellent .. |
|||
Density | 1.15 g/cc @Temperature 25.0 °C |
0.0415 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® 735 Rigid Polyol Description: Pluracol® 735 polyol is a modifying polyol which can be used in a wide variety of rigid foam applications and can be formulated using crude MDI, crude TDI, or TDI quasi-prepolymers. Fo.. |
|||
Density | 1.15 g/cc @Temperature 25.0 °C |
0.0415 lb/in³ @Temperature 77.0 °F |
|
BASF Pluracol® SG-450 Rigid Polyol Description: Pluracol® SG-450 polyol is a clear, light colored, sucrose/glycerine polyol. Pluracol SG-450 contains no nitrogen. The high sucrose content with the high hydroxyl number has excellent .. |
|||
Density | 1.15 g/cc @Temperature 25.0 °C |
0.0415 lb/in³ @Temperature 77.0 °F |
Part A; ASTM D1622 |
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive Redux® 810 is a multi-purpose, high shear and peel strength, two-part, toughened epoxy paste adhesive with corrosion-inhibiting properties.Features: Available in cartridges with a static mixer and .. |