Physical Properties Metric English Comments
Density 1.04 g/cc

@Temperature 40.0 °C
0.0376 lb/in³

@Temperature 104 °F
Concentration 0.10 kg HCl/kg
Solvay Chemicals Hydrochloric Acid 31% - Technical Grade (2 wt% - 10 wt% Concentration)
Hydrochloric acid, also known as muriatic acid, is a colorless to yellow liquid, with a pungent odor. Hydrochloric acid is a strong acid used as chemical reagent, pH-regulating, ion exchanger regene..
Density 1.04 g/cc

@Temperature 25.0 °C
0.0376 lb/in³

@Temperature 77.0 °F
BASF Pluracol® 1365 Graft Slabstock Foam Polyol
Description: Pluracol® 1365 polyol is a graft polyether polyol containing copolymerized styrene and acrylonitrile. This low functionality polyol is designed to produce flexible slabstock foams with..
Density 1.04 g/cc

@Temperature 30.0 °C
0.0376 lb/in³

@Temperature 86.0 °F
BASF Pluracol® 1365 Graft Slabstock Foam Polyol
Description: Pluracol® 1365 polyol is a graft polyether polyol containing copolymerized styrene and acrylonitrile. This low functionality polyol is designed to produce flexible slabstock foams with..
Density 1.04 g/cc

@Temperature 25.0 °C
0.0376 lb/in³

@Temperature 77.0 °F
BASF Pluracol® 4800 HR Foam Polyol
Description: Pluracol® 4800 polyol is a primary OH tipped copolymer polyol containing approximately 45% copolymerized styrene-acrylonitrile suitable for molded foam applications. Pluracol polyol 48..
Density 1.04 g/cc

@Temperature 40.0 °C
0.0376 lb/in³

@Temperature 104 °F
BASF Pluracol® 4800 HR Foam Polyol
Description: Pluracol® 4800 polyol is a primary OH tipped copolymer polyol containing approximately 45% copolymerized styrene-acrylonitrile suitable for molded foam applications. Pluracol polyol 48..
Density 1.04 g/cc

@Temperature 25.0 °C
0.0376 lb/in³

@Temperature 77.0 °F
BASF Pluracol® 4850 Slabstock HR & Molded Graft Polyol
Description: Pluracol® 4850 polyol is a primary hydroxyl-terminated graft polyether triol containing approximately 32% solids of copolymerized styrene and acrylonitrile, utilizing a LVI inhibitor p..
Density 1.04 g/cc

@Temperature 40.0 °C
0.0376 lb/in³

@Temperature 104 °F
BASF Pluracol® 736 Rigid Polyol
Description: Pluracol® 736 polyol is an aromatic initiator-based polyol which can be used in a variety of rigid foam formulations. This polyol can be reacted with crude MDI, crude TDI or TDI quasip..
Density 1.04 g/cc

@Temperature 37.8 °C
0.0376 lb/in³

@Temperature 100 °F
BASF Pluracol® GP 430R Specialty Polyol
Description: Pluracol® GP polyols are a series of four trifunctional polyols formed by adding propylene oxide to a glycerine nucleus. All Pluracol GP polyols are used in the preparation of polyure..
Density 1.04 g/cc

@Temperature 40.0 °C
0.0376 lb/in³

@Temperature 104 °F
BASF Pluracol® 5250 Graft Slabstock Foam Polyol
Description: Pluracol® 5250 polyol is a graft polyether triol containing copolymerized styrene and acrylonitrile. This secondary hydroxyl-terminated polyol contains approximately 50% solids. It is ..
Density 1.04 g/cc

@Temperature 25.0 °C
0.0376 lb/in³

@Temperature 77.0 °F
BASF Pluracol® GP 730 Specialty Polyol
Description: Pluracol® GP polyols are a series of four trifunctional polyols formed by adding propylene oxide to a glycerine nucleus. All Pluracol GP polyols are used in the preparation of polyure..