Material Notes:
Hydrochloric acid, also known as muriatic acid, is a colorless to yellow liquid, with a pungent odor. Hydrochloric acid is a strong acid used as chemical reagent, pH-regulating, ion exchanger regenerating, pickling or cleaning agent.EINECS: 231-595-7/CAS: 7647-01-0/UN: 1789Information provided by Solvay
Physical Properties Metric English Comments
Density 0.9639 g/cc

@Temperature 100 °C
0.03482 lb/in³

@Temperature 212 °F
Concentration 0.01 kg HCl/kg
0.9688 g/cc

@Temperature 100 °C
0.03500 lb/in³

@Temperature 212 °F
Concentration 0.02 kg HCl/kg
0.9791 g/cc

@Temperature 100 °C
0.03537 lb/in³

@Temperature 212 °F
Concentration 0.04 kg HCl/kg
0.9892 g/cc

@Temperature 100 °C
0.03574 lb/in³

@Temperature 212 °F
Concentration 0.06 kg HCl/kg
0.997 g/cc

@Temperature 40.0 °C
0.0360 lb/in³

@Temperature 104 °F
Concentration 0.01 kg HCl/kg
0.9992 g/cc

@Temperature 100 °C
0.03610 lb/in³

@Temperature 212 °F
Concentration 0.08 kg HCl/kg
1.0019 g/cc

@Temperature 40.0 °C
0.036196 lb/in³

@Temperature 104 °F
Concentration 0.02 kg HCl/kg
1.0048 g/cc

@Temperature -5.00 °C
0.036301 lb/in³

@Temperature 23.0 °F
Concentration 0.01 kg HCl/kg
1.009 g/cc

@Temperature 100 °C
0.03645 lb/in³

@Temperature 212 °F
Concentration 0.10 kg HCl/kg
1.0104 g/cc

@Temperature -5.00 °C
0.036503 lb/in³

@Temperature 23.0 °F
Concentration 0.02 kg HCl/kg
1.0116 g/cc

@Temperature 40.0 °C
0.036546 lb/in³

@Temperature 104 °F
Concentration 0.04 kg HCl/kg
1.0211 g/cc

@Temperature 40.0 °C
0.036890 lb/in³

@Temperature 104 °F
Concentration 0.06 kg HCl/kg
1.0213 g/cc

@Temperature -5.00 °C
0.036897 lb/in³

@Temperature 23.0 °F
Concentration 0.04 kg HCl/kg
1.0305 g/cc

@Temperature 40.0 °C
0.037229 lb/in³

@Temperature 104 °F
Concentration 0.08 kg HCl/kg
1.0321 g/cc

@Temperature -5.00 °C
0.037287 lb/in³

@Temperature 23.0 °F
Concentration 0.06 kg HCl/kg
1.04 g/cc

@Temperature 40.0 °C
0.0376 lb/in³

@Temperature 104 °F
Concentration 0.10 kg HCl/kg
1.0428 g/cc

@Temperature -5.00 °C
0.037674 lb/in³

@Temperature 23.0 °F
Concentration 0.08 kg HCl/kg
1.0536 g/cc

@Temperature -5.00 °C
0.038064 lb/in³

@Temperature 23.0 °F
Concentration 0.10 kg HCl/kg
Viscosity 0.30 cP

@Temperature 100 °C
0.30 cP

@Temperature 212 °F
Dynamic, Concentration 0.05 kg FeCl3/kg
0.31 cP

@Temperature 100 °C
0.31 cP

@Temperature 212 °F
Dynamic, Concentration 0.10 kg FeCl3/kg
0.38 cP

@Temperature 80.0 °C
0.38 cP

@Temperature 176 °F
Dynamic, Concentration 0.05 kg FeCl3/kg
0.41 cP

@Temperature 80.0 °C
0.41 cP

@Temperature 176 °F
Dynamic, Concentration 0.10 kg FeCl3/kg
0.51 cP

@Temperature 60.0 °C
0.51 cP

@Temperature 140 °F
Dynamic, Concentration 0.05 kg FeCl3/kg
0.56 cP

@Temperature 60.0 °C
0.56 cP

@Temperature 140 °F
Dynamic, Concentration 0.10 kg FeCl3/kg
0.72 cP

@Temperature 40.0 °C
0.72 cP

@Temperature 104 °F
Dynamic, Concentration 0.05 kg FeCl3/kg
0.79 cP

@Temperature 40.0 °C
0.79 cP

@Temperature 104 °F
Dynamic, Concentration 0.10 kg FeCl3/kg
1.1 cP

@Temperature 20.0 °C
1.1 cP

@Temperature 68.0 °F
Dynamic, Concentration 0.05 kg FeCl3/kg
1.19 cP

@Temperature 20.0 °C
1.19 cP

@Temperature 68.0 °F
Dynamic, Concentration 0.10 kg FeCl3/kg
1.4 cP

@Temperature 10.0 °C
1.4 cP

@Temperature 50.0 °F
Dynamic, Concentration 0.05 kg FeCl3/kg
1.5 cP

@Temperature 10.0 °C
1.5 cP

@Temperature 50.0 °F
Dynamic, Concentration 0.10 kg FeCl3/kg
1.84 cP

@Temperature 0.000 °C
1.84 cP

@Temperature 32.0 °F
Dynamic, Concentration 0.05 kg FeCl3/kg
1.94 cP

@Temperature 0.000 °C
1.94 cP

@Temperature 32.0 °F
Dynamic, Concentration 0.10 kg FeCl3/kg
2.58 cP

@Temperature -10.0 °C
2.58 cP

@Temperature 14.0 °F
Dynamic, Concentration 0.10 kg FeCl3/kg
Molecular Weight 36.47 g/mol
36.47 g/mol
HCl
Vapor Pressure 0.00200 bar

@Temperature -10.0 °C
1.50 torr

@Temperature 14.0 °F
Concentration 0.10 kg HCl/kg
0.00500 bar

@Temperature 0.000 °C
3.75 torr

@Temperature 32.0 °F
Concentration 0.10 kg HCl/kg
0.00600 bar

@Temperature 0.000 °C
4.50 torr

@Temperature 32.0 °F
Concentration 0.05 kg HCl/kg
0.0110 bar

@Temperature 10.0 °C
8.25 torr

@Temperature 50.0 °F
Concentration 0.10 kg HCl/kg
0.0120 bar

@Temperature 10.0 °C
9.00 torr

@Temperature 50.0 °F
Concentration 0.05 kg HCl/kg
0.0210 bar

@Temperature 20.0 °C
15.8 torr

@Temperature 68.0 °F
Concentration 0.10 kg HCl/kg
0.0220 bar

@Temperature 20.0 °C
16.5 torr

@Temperature 68.0 °F
Concentration 0.05 kg HCl/kg
0.0650 bar

@Temperature 40.0 °C
48.8 torr

@Temperature 104 °F
Concentration 0.10 kg HCl/kg
0.0700 bar

@Temperature 40.0 °C
52.5 torr

@Temperature 104 °F
Concentration 0.05 kg HCl/kg
0.170 bar

@Temperature 60.0 °C
128 torr

@Temperature 140 °F
Concentration 0.10 kg HCl/kg
0.190 bar

@Temperature 60.0 °C
143 torr

@Temperature 140 °F
Concentration 0.05 kg HCl/kg
0.410 bar

@Temperature 80.0 °C
308 torr

@Temperature 176 °F
Concentration 0.10 kg HCl/kg
0.450 bar

@Temperature 80.0 °C
338 torr

@Temperature 176 °F
Concentration 0.05 kg HCl/kg
0.890 bar

@Temperature 100 °C
668 torr

@Temperature 212 °F
Concentration 0.10 kg HCl/kg
0.970 bar

@Temperature 100 °C
728 torr

@Temperature 212 °F
Concentration 0.05 kg HCl/kg
Surface Tension 0.061 dynes/cm

@Temperature 100 °C
0.061 dynes/cm

@Temperature 212 °F
Concentration 0.05 HCl/kg
0.063 dynes/cm

@Temperature 100 °C
0.063 dynes/cm

@Temperature 212 °F
Concentration 0.10 HCl/kg
0.064 dynes/cm

@Temperature 80.0 °C
0.064 dynes/cm

@Temperature 176 °F
Concentration 0.05 HCl/kg
0.065 dynes/cm

@Temperature 80.0 °C
0.065 dynes/cm

@Temperature 176 °F
Concentration 0.10 HCl/kg
0.067 dynes/cm

@Temperature 60.0 °C
0.067 dynes/cm

@Temperature 140 °F
Concentration 0.05 HCl/kg
0.068 dynes/cm

@Temperature 60.0 °C
0.068 dynes/cm

@Temperature 140 °F
Concentration 0.10 HCl/kg
0.070 dynes/cm

@Temperature 40.0 °C
0.070 dynes/cm

@Temperature 104 °F
Concentration 0.05 HCl/kg
0.070 dynes/cm

@Temperature 40.0 °C
0.070 dynes/cm

@Temperature 104 °F
Concentration 0.10 HCl/kg
0.072 dynes/cm

@Temperature 20.0 °C
0.072 dynes/cm

@Temperature 68.0 °F
Concentration 0.10 HCl/kg
0.073 dynes/cm

@Temperature 10.0 °C
0.073 dynes/cm

@Temperature 50.0 °F
Concentration 0.10 HCl/kg
0.073 dynes/cm

@Temperature 20.0 °C
0.073 dynes/cm

@Temperature 68.0 °F
Concentration 0.05 HCl/kg
0.074 dynes/cm

@Temperature 0.000 °C
0.074 dynes/cm

@Temperature 32.0 °F
Concentration 0.10 HCl/kg
0.074 dynes/cm

@Temperature 10.0 °C
0.074 dynes/cm

@Temperature 50.0 °F
Concentration 0.05 HCl/kg
0.075 dynes/cm

@Temperature -10.0 °C
0.075 dynes/cm

@Temperature 14.0 °F
Concentration 0.10 HCl/kg
0.075 dynes/cm

@Temperature 0.000 °C
0.075 dynes/cm

@Temperature 32.0 °F
Concentration 0.05 HCl/kg
0.076 dynes/cm

@Temperature -10.0 °C
0.076 dynes/cm

@Temperature 14.0 °F
Concentration 0.05 HCl/kg