Physical Properties | Metric | English | Comments |
---|---|---|---|
Relative Viscosity | 2.37 cP | 2.37 cP | Correlation, Cyclohexanone 1%; Internal Method |
PolyOne Geon™ 130 Series 136 Polyvinyl Chloride Copolymer (PVC Copolymer) Geon® 136 is a vinyl ester copolymer dispersion resin, exhibiting fast fusion at low processing temperatures, resulting in energy saving and the ability to work with heat sensitive substrates. The .. |
|||
Relative Viscosity | 2.37 cP | 2.37 cP | 1% Cyclohexanone |
PolyOne Geon™ 170 Series 173 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Note: Plastisol Formulation F1 consists of 100 parts of this resin + 60 parts DOP. Note: Plastisol Formulation F2 consists of 100 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron®.. |
|||
Relative Viscosity | 2.37 cP | 2.37 cP | Correlation, Cyclohexanone 1%; Internal Method |
PolyOne Geon™ 170 Series L100UF Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Ultrafine 170-L100UF is a medium molecular weight, ultrafine particle size homopolymer dispersion resin. With the very fine particle size, it provides excellent casting characteristics for th.. |
|||
Relative Viscosity | 2.37 cP | 2.37 cP | Correlation, Cyclohexanone 1%; Internal Method |
PolyOne Geon™ Specialty Suspension Impel S100 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Impel S100 is a homopolymer specialty suspension resin intended for use in highly plasticized extrusion and injection molding formulations. It gives superior plasticizer absorption properties.. |
|||
Relative Viscosity | 2.37 cP | 2.37 cP | Correlation, Cyclohexanone 1%; Internal Method |
PolyOne Geon™ 120 Series 120X400 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 120X400 is medium molecular weight resin providing a good balance of fusion temperatures and film physical properties. It gives good chemical foamability for producing medium to high density .. |
|||
Relative Viscosity | 2.37 cP | 2.37 cP | Correlation, Cyclohexanone 1% |
PolyOne Geon™ 170 Series 174 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 174 is a medium molecular weight, fine particle size homopolymer dispersion resin. It provides a good balance of fused film properties and processing temperatures. It is recommended for appli.. |
|||
Relative Viscosity | 2.37 cP | 2.37 cP | |
Formosa Plastics Formolon® 680 PVC Homopolymer General Purpose Grade Resin F680 is especially suited for processing from powder blends due to its ability to rapidly absorb plasticizers regardless of molecular weight. In addition, thi.. |
|||
Relative Viscosity | 2.37 cP | 2.37 cP | |
Formosa Plastics Formolon® 680H PVC Homopolymer General Purpose Grade Resin F680H is especially suited for processing from powder blends due to its ability to rapidly absorb plasticizers regardless of molecular weight. In addition, th.. |
|||
Relative Viscosity | 2.37 cP | 2.37 cP | |
Formosa Plastics Formolon® 680M PVC Homopolymer General Purpose Grade Resin F680M is a medium molecular weight PVC homopolymer suitable for both rigid and flexible applications and is low in gels and finds acceptance in calendered fil.. |
|||
Relative Viscosity | 2.37 cP | 2.37 cP | |
Formosa Plastics Formolon® 685 PVC Homopolymer General Purpose Grade Resin F685 is especially suited for processing from powder blends due to its ability to absorb plasticizers regardless of molecular weight. In addition, this produc.. |