Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Density | 0.962 g/cc | 0.0348 lb/in³ | Melt density |
Styron Pulse® 759 ABS + Polycarbonate, 15% Glass Reinforced PULSE® 759 Engineering resin is a 15% glass reinforced resin designed to provide excellent processability, high heat resistance, and practical toughness. PULSE 759 Engineering resin has been used.. |
|||
Melt Density | 0.962 g/cc | 0.0348 lb/in³ | Melt density |
Styron Pulse® 830 ABS + Polycarbonate PULSE® 830 Engineering resin offers excellent processability, high heat resistance, and high impact strength at both room and low temperatures.PULSE 830 Engineering resin has been used in automot.. |