Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Mesh Size | 35 Mesh | 35 Mesh | less than 2%; ASTM D1921 |
Polimeros Mexicanos Rotolene® 93050 Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene for rotational molding. This resin is fully UV8 stabilized.Recommended for general purpose applications. Frequently used for water tanks (less tha.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | less than 2%; ASTM D1921 |
Polimeros Mexicanos Rotolene® 93835-TG Medium Density Polyethylene MDPE Copolymer with UV8 stabilizer in natural and colors.Recommended for rotomolding. Used for manufacture of water tanks > 2000 liters, cisterns, farm tanks, or tanks to contain strong acids and b.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | less than 2%; ASTM D1921 |
Polimeros Mexicanos Rotolene® Black Plus Polyethylene Polyethylene compound specially formulated for rotational molding applications requiring good mechanical properties and good mold release properties. Rotational molded parts have smooth surface and .. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | less than 2%; ASTM D1921 |
Polimeros Mexicanos Rotolene® Diesel Tank Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene. This resin is fully UV8 stabilized.High quality Polyethylene compound specially designed for automotive applications, water tanks, diesel tanks a.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | 2% |
Pau Tai UNINOX PA-401 PVC Processing Aid UNINOX PA-401 is a high molecular weight MMSAN (methyl methacrylate-styrene-acrylonitrile) processing aid. It is a cost effective processing aid for rigid PVC compounds such as calendered sheet, ext.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | 2% |
Pau Tai UNINOX PA-710 PVC Processing Aid UNINOX PA-710 is an acrylic lubricating process aid that offers significant berifits to processors of rigid PVC sheet, film, and molded products. This additive is designed to offer excellent clarity.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | 2% |
Pau Tai UNINOX AM-929 Acrylic Impact Modifier UNINOX AM-929 is acrylic impact modified resin. It is the most efficient high impact modifier for rigid PVC and other polymers, and recommended for use in calendered sheets, extruded pipe, foam prof.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | 95 wt% Passing |
Chevron Phillips Ryton® PR37 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | 85 wt% Passing |
Chevron Phillips Ryton® PR26 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | 95 wt% Passing |
Chevron Phillips Ryton® PR25 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | 85 wt% Passing |
Chevron Phillips Ryton® PR27 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | 85 wt% Passing |
Chevron Phillips Ryton® PR34 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | 85 wt% Passing |
Chevron Phillips Ryton® PR35 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | 95 wt% Passing |
Chevron Phillips Ryton® PR06 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | 85 wt% Passing |
Chevron Phillips Ryton® PR39 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | 95 wt% Passing |
Chevron Phillips Ryton® P-4 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | 95 wt% Passing |
Solvay Specialty Polymers Ryton® P-6 Polyphenylene Sulfide Coating Resin
(Unverified Data**) Characteristics: High temperatureNon-stickCorrosion resistantInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the Ryton product line. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | Irregular shape. ETM = Equistar Test Method; ETM Malvern |
LyondellBasell Microthene® G MN70100 Low Density Polyethylene General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | Irregular shape. ETM = Equistar Test Method; ETM Sieve Analysis |
LyondellBasell Microthene® G MN71120 Low Density Polyethylene (Rotomolding) General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | Irregular shape. ETM = Equistar Test Method; ETM Malvern |
LyondellBasell Microthene® G MU76000 Ethylene Vinyl Acetate Copolymer General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | Irregular shape. ETM = Equistar Test Method; ETM Malvern |
LyondellBasell Microthene® G MU76300 Ethylene Vinyl Acetate Copolymer General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | <2% (mesh on); LSY-QB-KD018 |
LG Chemical PA828 Processing aid Description: High molecular weightApplication: Foam, soft product etcInformation provided by LG Chemical |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | <2% (mesh on); LSY-QB-KD018 |
LG Chemical PA910 Processing aid Description: General purposeApplication: Sheet, window profile, pipe etcInformation provided by LG Chemical |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | <2% (mesh on); LSY-QB-KD018 |
LG Chemical PA930 Processing aid Description: Ultra high molecular weightApplication: Foam, soft product etcInformation provided by LG Chemical |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | max 3% |
H.C. Starck Amperweld® 1701.39 K1 Chromium Carbide RIII HS Number: 284990 |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | Opening 1700µm; ASTM E11 |
Solvay Chemicals SOLID CAUSTIC SODA MICROPEARLS Some applications of this product may be regulated or restricted by national or international standards (e.g. for food additives, water treatment, the pharmaceutical industry, etc). The buyer and th.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | 2% |
Pau Tai UNINOX PA-551 PVC Processing Aid UNINOX PA-551 is a high molecular weight acrylic polymer resin. This processing aid contributes greatly to rapid growth markets for rigid or flexible PVC compounds such as calendered sheet, extrusio.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | 99 wt% Passing |
Solvay Specialty Polymers Ryton® PR11 Polyphenylene Sulfide Resin
(Unverified Data**) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | 99.8 wt% Passing |
Solvay Specialty Polymers Ryton® V-1 Polyphenylene Sulfide Coating Resin
(Unverified Data**) Characteristics: High temperatureNon-stickCorrosion resistantApplications: CoatingsInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the Ryton product line. |
|||
Particle Mesh Size | 35 Mesh | 35 Mesh | 99 wt% Passing |
Chevron Phillips Ryton® PR11 Polyphenylene Sulfide Coating Resin
(Unverified Data**) Characteristics: High temperatureNon-stickCorrosion resistantInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the Ryton product line. |