Physical Properties Metric English Comments
Brookfield Viscosity 10000 - 60000 cP
10000 - 60000 cP
DOP 60phr, 6RPM; ASTM D1824
LG Chemical PE1311 PVC
General Description: PE1311, homopolymer made by emulsion polymerization, is a high-viscosity PVC resin with pseudo-plastic flow property PE1311 has an good chemical foaming with low density and fin..
Brookfield Viscosity <= 10000 cP
<= 10000 cP
#3 sp @ 12 rpm; RP-0596
Solvay MIRASHEEN® CP-820/G Surfactant
Description: New generation of ready to use, cost effective liquid pearl concentrate. A pumpable liquid that readily blends into formulated shampoos, liquid hand soaps, shower gels and related produ..
Brookfield Viscosity 10000 cP
10000 cP
20 rpm aged 2 hrs, See note 1; SPI-VD-T1
Formosa Plastics Formolon® 34 PVC
PVC Homopolymer Dispersion Resin F-34 is a medium molecular weight PVC homopolymer dispersion resin which has been developed primarily for use in chemically expanded compound. In expanded systems, t..
Brookfield Viscosity 10000 cP

@Temperature 25.0 °C
10000 cP

@Temperature 77.0 °F
Thixotropic
Loctite® 3103 Acrylic Light Cure Adhesive
Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co..
Brookfield Viscosity 10000 cP

@Temperature 25.0 °C
10000 cP

@Temperature 77.0 °F
Thixotropic
Loctite® 3211 Light Cure Acrylic Adhesive
Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe..
Brookfield Viscosity 10000 cP
10000 cP
2 rpm aged 2 hrs, See note 1; SPI-VD-T1
Formosa Plastics Formolon® 38 PVC
PVC Homopolymer Dispersion Resin F-38 is a high molecular weight PVC homopolymer dispersion resin which exhibits low paste viscosities, exceptional air release as well as a balance of other properti..
Brookfield Viscosity 10000 - 50000 cP
10000 - 50000 cP
RVF #16 sp @ 10 rpm
3M AC-236 Class A-2 Aerospace Sealant
3M Aerospace Sealant AC-236 Class A are brushable, two-component, liquid polysulfide polymer sealant providing excellent fuel tank and fuselage seals. They have outstanding resistance to aviation ga..
Brookfield Viscosity 10000 - 35000 cP
10000 - 35000 cP
Base, RVF #6 sp @ 10 rpm
3M AC-360 A-2 Aerospace Sealant
3M Aerospace Sealant AC-360 A-2 is a fast cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealant. 3M AC-360 A-2 Sealants maintain fle..
Brookfield Viscosity 10000 - 40000 cP
10000 - 40000 cP
Base, RVF #6 sp @ 10 rpm
3M Scotch-Weld™ DP640 Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-part, non-sag urethane adhesives. They feature tough, flexible bonds with good adhesion to a wide variety of substrates especially wood and many properl..
Brookfield Viscosity 10000 cP

@Temperature 23.9 °C
10000 cP

@Temperature 75.0 °F
Mixed
BCC Products BC 7053 Epoxy Casting
BC 7053 is an iron filled epoxy casting system. This system is a high iron content material that provides unsurpassed wear resistance. BC7053 was designed for use in constructing core boxes, holding..
Brookfield Viscosity 10000 cP
10000 cP
Catalyst
BCC Products BC 9020 Silicone RTV Rubber
BC 9020 is a violet colored, two-component, flowable compound that regardless of thickness or confinement, cures at room temperature. The cured rubber is high strength and high tear with good elonga..
Brookfield Viscosity 10000 cP
10000 cP
Mixed
BCC Products BC 9060 Silicone RTV Rubber
BC 9060 is a blue colored, two-component, flowable compound that, regardless of thickness or confinement, cures at room temperature or by application heat. The cured rubber is high strength and high..
Brookfield Viscosity 10000 - 55000 cP
10000 - 55000 cP
Base, RVF #6 sp @ 20 rpm
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Brookfield Viscosity 10000 - 40000 cP
10000 - 40000 cP
Base, RVF #6 sp @ 20 rpm
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..
Brookfield Viscosity 10000 - 50000 cP
10000 - 50000 cP
RVF #16 sp @ 10 rpm
3M AC-236 Class A-1/2 Aerospace Sealant
3M Aerospace Sealant AC-236 Class A are brushable, two-component, liquid polysulfide polymer sealant providing excellent fuel tank and fuselage seals. They have outstanding resistance to aviation ga..