Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 10000 - 60000 cP | 10000 - 60000 cP | DOP 60phr, 6RPM; ASTM D1824 |
LG Chemical PE1311 PVC General Description: PE1311, homopolymer made by emulsion polymerization, is a high-viscosity PVC resin with pseudo-plastic flow property PE1311 has an good chemical foaming with low density and fin.. |
|||
Brookfield Viscosity | <= 10000 cP | <= 10000 cP | #3 sp @ 12 rpm; RP-0596 |
Solvay MIRASHEEN® CP-820/G Surfactant Description: New generation of ready to use, cost effective liquid pearl concentrate. A pumpable liquid that readily blends into formulated shampoos, liquid hand soaps, shower gels and related produ.. |
|||
Brookfield Viscosity | 10000 cP | 10000 cP | 20 rpm aged 2 hrs, See note 1; SPI-VD-T1 |
Formosa Plastics Formolon® 34 PVC PVC Homopolymer Dispersion Resin F-34 is a medium molecular weight PVC homopolymer dispersion resin which has been developed primarily for use in chemically expanded compound. In expanded systems, t.. |
|||
Brookfield Viscosity | 10000 cP @Temperature 25.0 °C |
10000 cP @Temperature 77.0 °F |
Thixotropic |
Loctite® 3103 Acrylic Light Cure Adhesive Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co.. |
|||
Brookfield Viscosity | 10000 cP @Temperature 25.0 °C |
10000 cP @Temperature 77.0 °F |
Thixotropic |
Loctite® 3211 Light Cure Acrylic Adhesive Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe.. |
|||
Brookfield Viscosity | 10000 cP | 10000 cP | 2 rpm aged 2 hrs, See note 1; SPI-VD-T1 |
Formosa Plastics Formolon® 38 PVC PVC Homopolymer Dispersion Resin F-38 is a high molecular weight PVC homopolymer dispersion resin which exhibits low paste viscosities, exceptional air release as well as a balance of other properti.. |
|||
Brookfield Viscosity | 10000 - 50000 cP | 10000 - 50000 cP | RVF #16 sp @ 10 rpm |
3M AC-236 Class A-2 Aerospace Sealant 3M Aerospace Sealant AC-236 Class A are brushable, two-component, liquid polysulfide polymer sealant providing excellent fuel tank and fuselage seals. They have outstanding resistance to aviation ga.. |
|||
Brookfield Viscosity | 10000 - 35000 cP | 10000 - 35000 cP | Base, RVF #6 sp @ 10 rpm |
3M AC-360 A-2 Aerospace Sealant 3M Aerospace Sealant AC-360 A-2 is a fast cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealant. 3M AC-360 A-2 Sealants maintain fle.. |
|||
Brookfield Viscosity | 10000 - 40000 cP | 10000 - 40000 cP | Base, RVF #6 sp @ 10 rpm |
3M Scotch-Weld™ DP640 Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-part, non-sag urethane adhesives. They feature tough, flexible bonds with good adhesion to a wide variety of substrates especially wood and many properl.. |
|||
Brookfield Viscosity | 10000 cP @Temperature 23.9 °C |
10000 cP @Temperature 75.0 °F |
Mixed |
BCC Products BC 7053 Epoxy Casting BC 7053 is an iron filled epoxy casting system. This system is a high iron content material that provides unsurpassed wear resistance. BC7053 was designed for use in constructing core boxes, holding.. |
|||
Brookfield Viscosity | 10000 cP | 10000 cP | Catalyst |
BCC Products BC 9020 Silicone RTV Rubber BC 9020 is a violet colored, two-component, flowable compound that regardless of thickness or confinement, cures at room temperature. The cured rubber is high strength and high tear with good elonga.. |
|||
Brookfield Viscosity | 10000 cP | 10000 cP | Mixed |
BCC Products BC 9060 Silicone RTV Rubber BC 9060 is a blue colored, two-component, flowable compound that, regardless of thickness or confinement, cures at room temperature or by application heat. The cured rubber is high strength and high.. |
|||
Brookfield Viscosity | 10000 - 55000 cP | 10000 - 55000 cP | Base, RVF #6 sp @ 20 rpm |
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Brookfield Viscosity | 10000 - 40000 cP | 10000 - 40000 cP | Base, RVF #6 sp @ 20 rpm |
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Brookfield Viscosity | 10000 - 50000 cP | 10000 - 50000 cP | RVF #16 sp @ 10 rpm |
3M AC-236 Class A-1/2 Aerospace Sealant 3M Aerospace Sealant AC-236 Class A are brushable, two-component, liquid polysulfide polymer sealant providing excellent fuel tank and fuselage seals. They have outstanding resistance to aviation ga.. |