Physical Properties Metric English Comments
Oxygen Transmission Rate 20.2 cc/m²/day

@Temperature 23.0 °C
1.30 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Bicor™ 21MB777 OPP Film
Product Description: Bicor 21MB777 is a high gas barrier, biaxially oriented transparent PP film coated one side PVdC, one side acrylic. This film provides outstanding performance on all packaging m..
Oxygen Transmission Rate 20.2 cc/m²/day

@Temperature 23.0 °C
1.30 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Bicor™ 26MB768 OPP Film
Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side very low temperature seal (VLTS) coating. PVdC provides an excellent moi..
Oxygen Transmission Rate 20.2 cc/m²/day

@Temperature 23.0 °C
1.30 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Bicor™ 26MB777 OPP Film
Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side acrylic. This film provides outstanding performance on all packaging mac..
Oxygen Transmission Rate 20.2 cc/m²/day

@Temperature 23.0 °C
1.30 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Bicor™ 32MB768 OPP Film
Product Description: A High gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side very low temperature seal (VTLS) coating. PVdC provides excellent moistu..
Oxygen Transmission Rate 20.2 cc/m²/day

@Temperature 23.0 °C
1.30 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Bicor™ 32MB777 OPP Film
Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated one side PVdC, one side acrylic. This film provides outstanding performance on all packaging machin..
Oxygen Transmission Rate 20.2 cc/m²/day

@Temperature 23.0 °C
1.30 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Bicor™ 42MB777 OPP Film
Product Description: A high gas barrier, biaxially oriented transparent PP film, coated one side PVdC, one side acrylic, This film provides outstanding performance on all packaging machines.Availabi..
Oxygen Transmission Rate 20.2 cc/m²/day

@Temperature 23.0 °C
1.30 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 36MO747 OPP Film
Product Description: A white opaque biaxially oriented polypropylene film acrylic coated on one side, one side PVdC. Provides outstanding performances on all packaging machines.Availability: Africa ..
Oxygen Transmission Rate 20.2 cc/m²/day

@Temperature 23.0 °C
1.30 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 42AH748 OPP Film
Product Description: A high barrier, high speed, super white opaque, modified higher density biaxially oriented polypropylene film, coated one side high barrier PVdC, one side very low temperature s..
Oxygen Transmission Rate 20.2 cc/m²/day

@Temperature 23.0 °C
1.30 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 50MO747 OPP Film
Product Description: A white opaque biaxially oriented polypropylene film, coated on one side acrylic, one side PVdC. Provides excellent performance on all packaging machines.Availability: Africa & ..
Oxygen Transmission Rate 20.2 cc/m²/day

@Temperature 23.0 °C
1.30 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 30MW747 OPP Film
Product Description: White opaque biaxially oriented polypropylene film coated on one side acrylic, one side PVdC. Provides excellent performances on all packaging machines. 30MW747 is a super white..
Copyright © lookpolymers.com All Rights Reserved