Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 0.00800 cc-mm/m²-24hr-atm | 0.0203 cc-mil/100 in²-24hr-atm | 20°C- 65% RH; based on 20 µm layer |
Noltex Soarnol® D2908 Ethylene Vinyl Alcohol Copolymer Ethylene content 29 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a.. |
|||
Oxygen Transmission | 0.00800 cc-mm/m²-24hr-atm | 0.0203 cc-mil/100 in²-24hr-atm | 20°C- 65% RH; based on 20 µm layer |
Noltex Soarnol® DT2903 Ethylene Vinyl Alcohol Copolymer Very low ethylene content, high gas barrier for packaging dry products or for use in packaging material used at normal temperature and humidity. Ethylene content 29 mol%. Volatile matter 0.3%.The .. |
|||
Oxygen Transmission | 0.00800 cc-mm/m²-24hr-atm | 0.0203 cc-mil/100 in²-24hr-atm | 20°C; 65% RH; Permeability increases significantly at higher moisture content. |
EVALCA EVAL® F100 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a pa.. |
|||
Oxygen Transmission | 0.00800 cc-mm/m²-24hr-atm | 0.0203 cc-mil/100 in²-24hr-atm | 20°C; 65% RH; Permeability increases significantly at higher moisture content. |
EVALCA EVAL® LC-F101BZ Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, cast film, melt phase forming, blow molding, profile coextrusion. EVOH is used in packaging applications because of its outstan.. |
|||
Oxygen Transmission | 0.00800 cc-mm/m²-24hr-atm | 0.0203 cc-mil/100 in²-24hr-atm | 20°C; 65% RH; Permeability increases significantly at higher moisture content. |
EVALCA EVAL® EP-F104BW Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, blow molding, tubes, coex coating. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL.. |
|||
Oxygen Transmission | 0.00800 cc-mm/m²-24hr-atm | 0.0203 cc-mil/100 in²-24hr-atm | 20°C; 65% RH; Permeability increases significantly at higher moisture content. |
EVALCA EVAL® EF-F Ethylene Vinyl Alcohol Copolymer Film
(discontinued **) 32 mol % Ethylene. Non oriented type film; property values for 15 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pro.. |