Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.8 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.8 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
SABIC Innovative Plastics Geloy XTWM206 ASA Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 8.8 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.8 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
SABIC Innovative Plastics Geloy XTWM206 ASA (Asia Pacific) Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Asia Pacific regio.. |
|||
Melt Flow | 8.8 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.8 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
SABIC Innovative Plastics Geloy XTWM206 ASA (Europe-Africa-Middle East) Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Melt Flow | 8.8 g/10 min @Load 3.80 kg, Temperature 230 °C |
8.8 g/10 min @Load 8.38 lb, Temperature 446 °F |
Cond I; ASTM D1238 |
Ravago Manufacturing Americas Hylac® GP74 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Flow | 8.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
8.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem 1100FV PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Melt Flow | 8.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
8.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem 1100FV PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Melt Flow | 8.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
8.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem 1100FV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Melt Flow | 8.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
8.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem 1100V PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle Eas.. |