Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.3 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.3 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycolac® FR15U ABS Flame retardant ABS with excellent indoor UV properties and excellent processing. UL94 V-0/5VA rated. Elevated UL RTI rating (90-85-90) for all colors except for blue and green colors (60-60-60). |
|||
Melt Flow | 3.3 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.3 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycolac® FR15U ABS (Asia Pacific) Flame retardant ABS. Excellent indoor UV properties. Excellent moldability. UL94 V-0/5VA rated.ing. |
|||
Melt Flow | 3.3 g/10 min @Load 5.00 kg, Temperature 190 °C |
3.3 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) EX 2 S HF 7750 M2 High Density Polyethylene EX2S is a high density polyethylene with 1-Butene as co monomer. It is medium molar mass, low density grade with a narrow molar mass distribution, high rigidity, good tear strength. Applications: .. |
|||
Melt Flow | 3.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Chi Mei Polylac® PA-764 ABS - Flame Retardant F.R. Weather Resistant |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
ExxonMobil EXXELOR™ VA 1803 Maleic anhydride functionalized elastomeric ethylene copolymer Product Description: Exxelor VA 1803 polymer resin is a high flow, amorphous ethylene copolymer functionalized with maleic anhydride by reactive extrusion. Its fully saturated backbone results in ou.. |
|||
Melt Flow | 3.3 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.3 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS/PC 9801 Description: Injection Molding Grade, High Impact, High HeatInformation provided by Diamond Polymers, Inc. |