Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 17.4 g/10 min @Load 2.16 kg, Temperature 250 °C |
17.4 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Melt Flow | 17.4 g/10 min @Load 2.16 kg, Temperature 250 °C |
17.4 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Asia Pacific) Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Melt Flow | 17.4 g/10 min @Load 2.16 kg, Temperature 250 °C |
17.4 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Europe-Africa-Middle East) Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Melt Flow | 17.4 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.4 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP THERMOCOMP D452 PC COPOLYMER (Asia Pacific) LNP* Thermocomp* D452 (or EXTC8202) is a compound based on SABIC unique Polycarbonate copolymer resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, .. |