Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
SABIC B4660/B4660AB High Density Polyethylene for Blow Molding Product Description: B4660 series grades are medium molecular weight High Density Polyethylene homopolymer for blow molding applications. They are primarily designed for imparting high rigidity, t.. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
SABIC F04660 High Density Polyethylene for Blown Film Applications Product Description: F04660 is a homopolymer HDPE film grade with excellent processability and high stiffness. It has good moisture barrier properties and can be blended with LDPE and LLDPE to imp.. |
|||
Melt Flow | 0.70 g/10 min @Load 1.00 kg, Temperature 235 °C |
0.70 g/10 min @Load 2.20 lb, Temperature 455 °F |
Procedure A Condition Q; ASTM D1238 |
Network Polymers Softflex® 6500 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 0.70 - 0.90 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 - 0.90 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 6348M (486F8) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.70 - 0.90 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.70 - 0.90 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 6750H (506H8) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® PF 92 High Density Polyethylene - Pipe Grade Resin Eraclene PF 92 is a homopolymer high density polyethylene resin (HDPE) with antioxidants, suitable for pipe application. It is characterized by high rigidity, high impact strength and low swelling... |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
SABIC BM6246LS High Density Polyethylene for Blow Molding Product Description: BM6246LS grade is a medium molecular weight High Density Polyethylene homopolymer for blow molding applications. It is primarily designed for imparting high rigidity, toughnes.. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg |
0.70 g/10 min @Load 4.76 lb |
ISO 1133 |
Total Lacqtene® 2006 PBK 35 HDPE pipe, sheet
(discontinued **) LACQTENE® 2006 PBK 35 is a medium density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2006 PBK 35 may be used for pipe extrusion (micro-irriga.. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg |
0.70 g/10 min @Load 4.76 lb |
ISO 1133 |
Total Lacqtene® 2007 TN 61 HDPE pipe
(discontinued **) LACQTENE® 2007 TN 61 is a high density homopolymer polyethylene produced by the gas phase polymerization process.LACQTENE® 2007 TN 61 is best processed between 190 and 230°C.Information provided .. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg |
0.70 g/10 min @Load 4.76 lb |
ISO 1133 |
Total Lacqtene® 2006 TN 35 HDPE pipe coating
(discontinued **) LACQTENE® 2006 TN 35 is a medium density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2006 TN 35 may be used for pipe and sheet extrusion (flex.. |
|||
Melt Flow | 0.70 g/10 min @Load 3.80 kg, Temperature 230 °C |
0.70 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM-D1238, ISO 1133 |
Ineos ABS Lustran® Guardian™ 682 ABS, Injection Molding Grade Lustran® ABS 682 is a high performance, HCFC-141b resistant grade of ABS for injection molded refrigerator and freezer components. |
|||
Melt Flow | 0.70 - 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 - 1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
±10% |
Kazanorgsintez PE2NT 15-10 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Melt Flow | 0.70 - 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 - 1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
±10% |
Kazanorgsintez PE2NT 15-5 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Melt Flow | 0.70 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.70 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borstar® FB1350 Medium Density Polyethylene Borstar® FB1350 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Borstar® FB1350 is well suited for mono- and coextrusion of films .. |
|||
Melt Flow | 0.70 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.70 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® BB 29 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 0.70 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.70 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® BB 85 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® FB 29 HDPE Made for tubular film applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® FB 85 HDPE Made for tubular film applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® VL 20 HDPE Extrusion and pipe applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis BS4641 High Density Polyethylene BS4641 is a bimodal high-density polyethylene homopolymer. Because of its excellent organoleptic properties, this grade is especially suitable for blow molding of bottles for food applications. App.. |
|||
Melt Flow | 0.70 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.70 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil HDPE HYA 800 High Density Polyethylene Resin Product Description: HYA 800 is a homopolymer HDPE grade, characterized by high stiffness, high rigidity and high flow.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal .. |
|||
Melt Flow | 0.70 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.70 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Denka TX-400S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Melt Flow | 0.70 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.70 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers ABS 3501 Natural 1002 ESCR Injection Molding Grade, Environmental Stress Crack Resistant Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 0.70 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.70 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers ABS 3501E Natural 1002 ESCR Extrusion Grade, Environmental Stress Crack Resistant Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 0.70 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.70 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers ABS 3501ELG High Impact, Low Gloss Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 0.70 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.70 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS TM 35 Description: Heat Resistant Grade, Ultra High HeatInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.70 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.70 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ASA T-120 Description: ASA Weatherable Polymer, Injection Molding Grade, High Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.70 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.70 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ASA/PC FA-30 Description: ASA Weatherable Polymer, Injection Molding Grade, Flame RetardantInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.70 g/10 min @Load 10.0 kg, Temperature 220 °C |
0.70 g/10 min @Load 22.0 lb, Temperature 428 °F |
Procedure A; ASTM D1238 |
Diamond Polymers SE 3 HH Description: High Heat ABSInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.70 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.70 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem BS600 HDPE Blow Molding Polyethylene Copolymer BS600 resin is a high-density polyethylene (HDPE), bimodal copolymer offering an outstanding combination of impact resistance and environmental stress crack resistance (ESCR). It is thus recommended.. |