Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.35 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.35 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
SABIC FI1157 Bimodal High Density Polyethylene for Blown Film Product Description: FI1157 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Melt Flow | 0.35 - 0.45 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.35 - 0.45 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4131L (314F4) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.35 g/10 min @Load 5.00 kg |
0.35 g/10 min @Load 11.0 lb |
ISO 1133 |
Total Finathene® 1288 HDPE film
(discontinued **) Applications: Flat bottom bags, draw strings, coextruded merchandise bags, deli wrapInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plasti.. |
|||
Melt Flow | 0.35 - 0.70 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.35 - 0.70 g/10 min @Load 11.0 lb, Temperature 374 °F |
±10% |
Kazanorgsintez PE80B-275 Medium Density Polyethylene Composite Production Method: Copolymerization of ethylene at low pressure using advanced technology and in presence of complex catalysts on carrier material that allows production of polyethylene with enhanc.. |
|||
Melt Flow | 0.35 - 0.70 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.35 - 0.70 g/10 min @Load 11.0 lb, Temperature 374 °F |
±10% |
Kazanorgsintez PE80B-286 Medium Density Polyethylene Composite Production Method: Copolymerization of ethylene at low pressure using advanced technology and in presence of complex catalysts on carrier material that allows production of polyethylene with enhanc.. |
|||
Melt Flow | 0.35 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.35 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) BL 4M HM 8355 High Density Polyethylene BL4M is a high density polyethylene with 1-Butene as co monomer. It is high molar mass, easily processable, high stiffness and strength, good SCR, very good molding surface finish.Applications: jer.. |
|||
Melt Flow | 0.35 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.35 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) BL4 HM 8255 High Density Polyethylene BL4 (HM 8255) is a high density polyethylene with Butene-1 as comonomer. It is a high molar mass, easily processable, high stiffness and impact good stress cracking resistance and even good molding .. |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
IRPC Polimaxx Polene G2855 High Density Polyethylene CHARACTERISTICS:GOOD IMPACT STRENGTH, MEDUIM STIFFNESSGOOD PROCESSABILITYAPPLICATIONS:BLOW MOLDINGFOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, LUBRICANT BOTTLES,COSMETIC BOTTLES, CHEMICAL CONTAI.. |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
IRPC Polimaxx Polene G2865 High Density Polyethylene CHARACTERISTICS: HIGH STIFFNESS, GOOD IMPACT STRENGTH, GOOD PROCESSABILITYAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, DIARY PRODUCT BOTTLES, FRUIT JUICE BOTTLES, ONE-.. |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
IRPC Polimaxx Polene GM2860 High Density Polyethylene CHARACTERISTICS: HIGH IMPACT STRENGTH, GOOD PROCESSABILITY, HIGH STIFFNESSAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, LUBRICANT BOTTLES COSMETIC BOTTLES, ONE-WAY BOTT.. |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
IRPC Polimaxx Polene GM2865 High Density Polyethylene CHARACTERISTICS: EXCELLENT STIFFNESS, GOOD PROCESSABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, DAIRY PRODUCT BOTTLES MILK BOTTLES AND GALL.. |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Total HDPE HL 535 High Density Polyethylene, Film Resin Polyethylene: Medium molecular weight, high density film resinCharacteristics:High stiffnessGood heat resistanceExcellent bubble stabilityGood compatibility with LDPE and LLDPEApplications:Release .. |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil HDPE HYA 600 High Density Polyethylene Resin Product Description: HYA 600 is a general purpose HDPE resin, characterized by very easy processability, an excellent balance of rigidity and impact strength and a good ESCR.Availability: Africa & M.. |
|||
Melt Flow | 0.35 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.35 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ASA S519 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.35 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem BS002HS HDPE Blow Molding Polyethylene Copolymer Resin BS002HS is a high-density polyethylene, bimodal copolymer. It presents good rigidity, good impact resistance, and good reproducibility of the weight of the bottles. It also has excellent envir.. |