Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Vapor Pressure = 300 torr Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Vapor Pressure 0.400 bar
300 torr
Solvay Chemicals Allyl chloride 3-chloropropene
Allyl chloride is mainly used in the manufacture of epichlorohydrin. It is also used in the production of allylic ethers, esters, silanes and quaternary ammonium derivatives.EINECS Number: 203-457-6..
Vapor Pressure 0.400 bar
300 torr
Solvay Chemicals Allyl chloride High purity – Non stabilized 3-chloropropene
Allyl chloride is mainly used in the manufacture of epichlorohydrin. It is also used in the production of allylic ethers, esters, silanes and quaternary ammonium derivatives.EINECS Number: 203-457-6..
Vapor Pressure 0.400 bar
300 torr
Solvay Chemicals Allyl chloride High purity 3-chloropropene
Allyl chloride is mainly used in the manufacture of epichlorohydrin. It is also used in the production of allylic ethers, esters, silanes and quaternary ammonium derivatives.EINECS Number: 203-457-6..
Vapor Pressure 0.400 bar
300 torr
3M Novec™ 649 Engineered Fluid
3M™ Novec™ 649 Engineered Fluid is a clear, colorless and low odor fluid, one in a line of 3M products designed as replacements for ozone depleting substances (ODSs) and compounds with high global..
Copyright © lookpolymers.com All Rights Reserved