| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.7911 g/cc @Pressure 0.7726 MPa, Temperature 120 °C |
0.02858 lb/in³ @Pressure 112.1 psi, Temperature 248 °F |
|
| 0.8084 g/cc @Pressure 0.6201 MPa, Temperature 110 °C |
0.02921 lb/in³ @Pressure 89.94 psi, Temperature 230 °F |
||
| 0.825 g/cc @Pressure 0.4912 MPa, Temperature 100 °C |
0.0298 lb/in³ @Pressure 71.24 psi, Temperature 212 °F |
||
| 0.8411 g/cc @Pressure 0.3835 MPa, Temperature 90.0 °C |
0.03039 lb/in³ @Pressure 55.62 psi, Temperature 194 °F |
||
| 0.8565 g/cc @Pressure 0.2947 MPa, Temperature 80.0 °C |
0.03094 lb/in³ @Pressure 42.74 psi, Temperature 176 °F |
||
| 0.8714 g/cc @Pressure 0.2226 MPa, Temperature 70.0 °C |
0.03148 lb/in³ @Pressure 32.29 psi, Temperature 158 °F |
||
| 0.8859 g/cc @Pressure 0.1649 MPa, Temperature 60.0 °C |
0.03201 lb/in³ @Pressure 23.92 psi, Temperature 140 °F |
||
| 0.8999 g/cc @Pressure 0.1196 MPa, Temperature 50.0 °C |
0.03251 lb/in³ @Pressure 17.35 psi, Temperature 122 °F |
||
| 0.9136 g/cc @Pressure 0.0848 MPa, Temperature 40.0 °C |
0.03301 lb/in³ @Pressure 12.3 psi, Temperature 104 °F |
||
| 0.9203 g/cc @Pressure 0.0707 MPa, Temperature 35.0 °C |
0.03325 lb/in³ @Pressure 10.3 psi, Temperature 95.0 °F |
||
| 0.9269 g/cc @Pressure 0.0585 MPa, Temperature 30.0 °C |
0.03349 lb/in³ @Pressure 8.48 psi, Temperature 86.0 °F |
||
| 0.9334 g/cc @Pressure 0.0481 MPa, Temperature 25.0 °C |
0.03372 lb/in³ @Pressure 6.98 psi, Temperature 77.0 °F |
||
| 0.9398 g/cc @Pressure 0.0392 MPa, Temperature 20.0 °C |
0.03395 lb/in³ @Pressure 5.69 psi, Temperature 68.0 °F |
||
| 0.9462 g/cc @Pressure 0.0317 MPa, Temperature 15.0 °C |
0.03418 lb/in³ @Pressure 4.60 psi, Temperature 59.0 °F |
||
| 0.9525 g/cc @Pressure 0.0254 MPa, Temperature 10.0 °C |
0.03441 lb/in³ @Pressure 3.68 psi, Temperature 50.0 °F |
||
| 0.9587 g/cc @Pressure 0.0202 MPa, Temperature 5.00 °C |
0.03464 lb/in³ @Pressure 2.93 psi, Temperature 41.0 °F |
||
| 0.9648 g/cc @Pressure 0.0159 MPa, Temperature 0.000 °C |
0.03486 lb/in³ @Pressure 2.31 psi, Temperature 32.0 °F |
||
| 0.9709 g/cc @Pressure 0.0124 MPa, Temperature -5.00 °C |
0.03508 lb/in³ @Pressure 1.80 psi, Temperature 23.0 °F |
||
| 0.9769 g/cc @Pressure 0.00950 MPa, Temperature -10.0 °C |
0.03529 lb/in³ @Pressure 1.38 psi, Temperature 14.0 °F |
||
| 0.9828 g/cc @Pressure 0.00720 MPa, Temperature -15.0 °C |
0.03551 lb/in³ @Pressure 1.04 psi, Temperature 5.00 °F |
||
| 0.9887 g/cc @Pressure 0.00540 MPa, Temperature -20.0 °C |
0.03572 lb/in³ @Pressure 0.783 psi, Temperature -4.00 °F |
||
| 1.0003 g/cc @Pressure 0.00290 MPa, Temperature -30.0 °C |
0.036138 lb/in³ @Pressure 0.421 psi, Temperature -22.0 °F |
||
| Solubility in Water | 0.36 % | 0.36 % | |
| Viscosity | 0.34 cP | 0.34 cP | |
| Molecular Weight | 76.53 g/mol | 76.53 g/mol | |
| Vapor Pressure | 0.400 bar | 300 torr | |
| Surface Tension | 0.023 dynes/cm | 0.023 dynes/cm |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Heat Capacity | 0.950 J/g-°C | 0.227 BTU/lb-°F | vapor |
| 1.50 J/g-°C | 0.359 BTU/lb-°F | liquid | |
| Melting Point | -135 °C | -211 °F | Freezing Point |
| Boiling Point | 43.0 °C | 109 °F | Azeotrope with water |
| 45.0 °C @Pressure 1.013 MPa |
113 °F @Pressure 146.9 psi |
||
| Decomposition Temperature | >= 80.0 °C | >= 176 °F | |
| Flash Point | -27.0 °C | -16.6 °F | TAG closed cup |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 1.013 @Temperature 19.0 °C |
1.013 @Temperature 66.2 °F |
vapor |
| 8.2 @Temperature 20.0 °C |
8.2 @Temperature 68.0 °F |
liquid |
| Chemical Properties | Metric | English | Comments |
|---|---|---|---|
| Critical Pressure | 48.0 bar | 36000 torr | |
| Critical Temperature | 241 °C | 466 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Clear liquid, free from visible matter or particles | |
| Auto-ignition temperature | >392°C | |
| Coefficient of volume expansion | 0.0014 | K<sup>-1</sup> |
| Combustion heat | 24 kJ/g | |
| Composition | <200 mg/kg | Water, ASTM D3401, ASTM E1064 |
| >98% | Allyl Chloride - assay | |
| 0.5-90.9 g/kg | Stabilizer | |
| 22 g/kg | Azetrope with water, content | |
| Flammability limits | 3.3-11.2% | |
| Latent heat of evaporation | 0.37 kJ/g | 45°C |
| Partition coefficient P | 2.1 Log P o/w | n-octanol.water |
| Solubility of water in organic | 0.8 g/kg |