Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 114 - 165 microns | 4.50 - 6.50 mil | Overall |
Arlon 48571R005 0.0055" (0.140 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specif.. |
|||
Thickness | 114 - 165 microns | 4.50 - 6.50 mil | Overall |
Arlon 48576R005 0.0055" (0.140 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured RubberSide 2: Uncured RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specific.. |
|||
Thickness | 88.9 - 165 microns | 3.50 - 6.50 mil | Side 1 |
Arlon 47091R012 0.012" (0.305 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data should not be u.. |
|||
Thickness | 127 - 165 microns | 5.00 - 6.50 mil | Overall |
Arlon R32861R006 0.0055" (0.140 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Rubber Side 2: Uncured Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material spec.. |
|||
Thickness | 140 - 165 microns | 5.50 - 6.50 mil | Film and adhesive |
3M 3635-100 Light Enhancement Film A light box or channel letter contains lighting elements that illuminate the front sign face and transmit some light to the viewer. However much of the illumination is reflected or absorbed by other.. |
|||
Thickness | 127 - 165 microns | 5.00 - 6.50 mil | Overall |
Arlon 42561R006 0.0055" (0.140 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Rubber Side 2: RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specificationsInforma.. |
|||
Thickness | 127 - 165 microns | 5.00 - 6.50 mil | Overall |
Arlon 48571R006 0.0055" (0.140 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specif.. |