Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 191 - 343 microns | 7.50 - 13.5 mil | Urethane Foam |
Rogers Corporation Poron® 4790-79SP-15012 Urethane Shock Pad Foam Information provided by Rogers Corporation. |
|||
Thickness | 267 - 343 microns | 10.5 - 13.5 mil | Overall |
Arlon 47091R012 0.012" (0.305 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data should not be u.. |