Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 762 - 1520 microns | 30.0 - 60.0 mil | Range of Thicknesses Available |
Rogers Corporation RO3730 Antenna Grade Laminate RO3730™ Laminates have the excellent thermo-mechanical properties and electrical characteristics that antenna designers need. The laminates have a dielectric constant of 3.0 and a loss tangent of.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-012 |
Arlon A1030-R008-12 0.030" (0.762 mm) Fully Cured Fusible Silicone Rubber - Extruded Fusible Tape
(disco 2 inches width and 36 inches long. Design/Construction: Interleave: Polyester Film Extruded Fusible Tape (Rectangular Cross Section): Fully Cured Fusible Silicone RubberThis data represents typical.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-012 |
Arlon A1030-X008-12 0.030" (0.762 mm) Fully Cured Fusible Silicone Rubber - Extruded Fusible Tape
(disco 1 inch width and 36 inches long. Design/Construction: Interleave: Polyester Film Extruded Fusible Tape (Rectangular Cross Section): Fully Cured Fusible Silicone RubberThis data represents typical v.. |
|||
Thickness | 762 microns | 30.0 mil | |
Mid-Mountain Materials ARMATEX® SRS 28 Silica Fabric Coated with Silicone Rubber ARMATEX® SRS 28 is a silica fabric coated with silicone rubber on one or both sides to a finished weight of 28 oz/sq yd. An ideal product for heavy duty protection of equipment and personnel, ARM.. |
|||
Thickness | 762 microns | 30.0 mil | Nominal |
DuPont™ Nomex® 410 Paper, 30 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Thickness | 762 microns | 30.0 mil | Silicone |
Arlon 41400R030 0.030" Uncured, Unsupported Silicone Rubber on a Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 49481R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1681 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical .. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55576R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Uncured Silicone Rubber Interleave: LDPE This data represents typical values for the production material. T.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55586R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneAppearance: Red silicone gum and rubber on fiberglass clothTh.. |
|||
Thickness | 762 - 838 microns | 30.0 - 33.0 mil | Overall |
Arlon 55596R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55638R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater SubstrateAppearance: Red silic.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55946C030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: 162 Style Fiberglass Side 1: Cured Silicone Rubber This data represents typical values for the production mate.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 930-10Bxx-P0 0.030" (0.762 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 30 mil thick, Black, Rectangular cross-section, Self-fu.. |
|||
Thickness | 762 microns | 30.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon HSLW301R##-P0 0.030" (0.762 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: High Strength, 1 inch wide, 30 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicate.. |
|||
Thickness | 762 microns | 30.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon LW301CxxFR-P0 0.030" (0.762 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 30 mil thick, Brown, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon P3272-10Rxx-P4 0.030" (0.762 mm) Cured Self-Fusing Silicone Tape (Rectangular, Unsupported) Description: High strength self-fusing silicone tapeDesign/Construction: Interleave: PolyethyleneRubber: Cured Self-Fusing Silicone Rubber Cross-Section: 1” wide RectangularAppearance: Red silicone.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R30960T030 0.030" (0.762 mm) Uncured Silicone Rubber with Kodacel Substrate Design/Construction:Interleave: PolyethyleneAdd-on: Uncured Silicone Rubber Substrate: Kodacel CarrierAppearance: Translucent, high viscosity gum on release linersThis data represents typical values.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-012 |
Arlon T3030-R004 0.030" (0.762 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate Design/Construction: Side 1: Cured Fusible Silicone RubberSubstrate: 25% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester FilmArlon MOX-Tape® Fiberglass Reinforced T.. |
|||
Thickness | 762 microns | 30.0 mil | |
3M Scotchkote™ HTX 517 Epoxy HT Lining Scotchkote Epoxy HT Lining HTX 517 has been specifically developed as a 100% solids epoxy coating for resurfacing and lining equipment operating at high temperatures.Product Features:Combines good a.. |
|||
Thickness | 762 microns | 30.0 mil | Silicone |
Arlon 41580R030 0.030" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 51946C030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 1: Cured Silicone Wash Coat Appearance: Brown silicone rubber and gum on fiberglass.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55103R030 0.030" (0.762 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Cured Silicone Rubber This data represents typical values for the production materia.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55106R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silic.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R38081R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassSide 2: Uncured SiliconeInterleave 2: Polyethylene This data represents typical values .. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R38726R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured SiliconeThis data represents typical values for the production material. The.. |
|||
Thickness | 762 microns | 30.0 mil | |
3M Scotch® 77 White Fire-Retardant Electric Arc Proofing Tape Scotch® Fire-Retardant Electric Arc Proofing Tape 77 Series are designed to protect most types of electrical cables from fault arc-generated heat and flames of nearby cable failures. These elastome.. |
|||
Thickness | 762 microns | 30.0 mil | Silicone; Arlon SQA-TMS-003 |
Arlon 32580R030 0.030" Uncured Silicone Rubber on PET Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberCarrier: 0.005" PETThis data represents typical values for the production material and should not be used as mate.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 44141R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Clear PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Blue PolyethyleneThis data represent.. |
|||
Thickness | 762 microns | 30.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 55276R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Cured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silic.. |
|||
Thickness | 762 microns | 30.0 mil | overall; Arlon SQA-TMS-003 |
Arlon R37806X030 Silicone Rubber/Fiberglass Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber |