Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 100 microns | 3.94 mil | |
Premix Thermoplastics PREFLEX E100 Polyphenylene Ether (PPO/PPE) PREFLEX films combine outstanding dielectric properties, good heat stability, low water absorption and chemical resistance in a way not available before. Also rigid boards made of the same material .. |
|||
Thickness | >= 100 microns | >= 3.94 mil | Bondline thickness |
Parker Chomerics THERM-A-GAP™ GEL 30 High Performance Fully Cured Dispensable Gel Description: Parker Chomerics fully cured dispensable GELs eliminate time consuming hand assembly, decreasing installation costs and reducing customer manufacturing and purchasing (logistical) compl.. |
|||
Thickness | 100 microns | 3.94 mil | Standard |
GrafTech eGRAF® SPREADERSHIELD™ SS600 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Thickness | 100 - 127 microns | 3.94 - 5.00 mil | Available Range |
GrafTech eGRAF® SPREADERSHIELD™ SS600 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Thickness | >= 100 microns | >= 3.94 mil | Minimum Web |
GrafTech GRAFCELL® FFP-100 SERIES Flow Field Plate Graphite Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid.. |
|||
Thickness | 100 microns | 3.94 mil | As Tested |
Solvay Specialty Polymers Ajedium™ Film Thermoplastic Polyimide (PI, TP) TPI is a thermoplastic polyimide film that has excellent, thermal, chemical, electrical and physical properties. With a continuous use temperature to 240°C (465°F), TPI films offer superior ra.. |
|||
Thickness | 100 microns | 3.94 mil | |
Shandong Dongyue Shenzhou New Material Co CHFM 100 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM) Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th.. |
|||
Thickness | 100 microns | 3.94 mil | |
Topas Advanced Polymers TOPAS® 9903D-10 Cyclic Olefin Copolymer (COC) TOPAS® 9903D-10 is a very low glass transition temperature (Tg=33°C) film extrusion grade. It is designed to deliver high shrinkage at low temperatures in shrink packaging applications. It is a mo.. |
|||
Thickness | <= 100 microns | <= 3.94 mil | Per single coat |
Daikin NEOFLON AC-5600 PFA Coating Powder, White NEOFLON PFA coating powder is designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: Up to a thickness of 100 microns per single coat.Proces.. |
|||
Thickness | <= 100 microns | <= 3.94 mil | Per single coat |
Daikin NEOFLON NC-1500 FEP Coating Powder, White NEOFLON FEP coating powders are designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: Up to a thickness of 100 microns per single coat.Proc.. |
|||
Thickness | 100 microns | 3.94 mil | Typical Wall Thickness |
COI Ceramics Al2O3SiO2 Oxide Hollow Spheres Description: COI Ceramics, Inc. can fabricate a variety of thin shell hollow spheres of various compositions and sizes. These products are called Holospheres. They are available as loose spheres tha.. |
|||
Thickness | 100 microns | 3.94 mil | Typical Wall Thickness |
COI Ceramics SiC Hollow Spheres Description: COI Ceramics, Inc. can fabricate a variety of thin shell hollow spheres of various compositions and sizes. These products are called Holospheres. They are available as loose spheres tha.. |
|||
Thickness | 100 microns | 3.94 mil | |
Carmel Olefins IPETHENE® 100 Low Density Polyethylene IPETHENE® 100 is a low density polyethylene extrusion grade. It exhibits good impact and puncture resistance, good processability and good ESCR. APPLICATIONS IPETHENE® 100 is used for production.. |
|||
Thickness | 100 microns | 3.94 mil | |
Carmel Olefins IPETHENE® 4203 Low Density Polyethylene IPETHENE® 4203 is a low density polyethylene extrusion grade. It exhibits good impact and puncture resistance, very good bubble stability in thick-gauge blown film processing, and excellent ESCR. .. |
|||
Thickness | 100 - 140 microns | 3.94 - 5.51 mil | |
P & P Technology NF32B050A21 Nylon/PET/Cu+Ni Conductive Fabric P & P Technology material reference NF32B050A21 is a metalised conductive fabric designed for use in EMC shielding and in the manufacture of conductive EMC gaskets. The material is a rip-stop weave .. |