COI Ceramics SiC Hollow Spheres

Category Ceramic , Carbide
Manufacturer COI Ceramics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF COI Ceramics SiC Hollow Spheres.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: COI Ceramics, Inc. can fabricate a variety of thin shell hollow spheres of various compositions and sizes. These products are called Holospheres. They are available as loose spheres that can be added to a variety of end-user products. The spheres can also be bonded together and machined into products that are useful for various applications, or they may be bonded to other materials to produce hybrid articles. Applications: Include thermal barrier layers for combustor liners, structural insulation for thermal protection systems, or structural cores in combination with CMCs to create engineered components.Information from COI Ceramics, Inc.
Physical Properties Metric English Comments
Thickness 100 microns
3.94 mil
Typical Wall Thickness
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 1600 °C
2910 °F
Descriptive Properties Value Comments
Standard Sizes (mm) 4