Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 76.2 microns | 3.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon R35551X014 0.014" (0.356 mm) Uncured Rubber with Coated Nextel Substrate
(discontinued **) Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberSubstrate: Coated Nextel This data Represents typical values for the production material. The data should not be used to write, or in .. |
|||
Thickness | 76.2 microns | 3.00 mil | Liner; Arlon SQA-TMS-003 |
Arlon 10292R062 Cured Silicone Rubber (Unsupported) with Polyethylene Liner Design/Construction:Material: Cured Silicone RubberLiner: PolyethyleneRecommended Cure Cycle: Product delivered curedRecommended Post Cure Cycle: Product delivered post-curedAppearance: Red silicone.. |
|||
Thickness | 76.2 microns | 3.00 mil | Polyethylene, Interleave |
Arlon 49576R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mat.. |
|||
Thickness | 76.2 microns | 3.00 mil | Polyethylene, Interleave |
Arlon 51586R035 0.035" (0.889 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mate.. |
|||
Thickness | 76.2 microns | 3.00 mil | Interleave 1 |
Arlon 51581R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Red silicone gu.. |
|||
Thickness | 76.2 microns | 3.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 51986R015 0.0165" (0.419 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flexible heater substrateAppearance: Red colo.. |
|||
Thickness | 76.2 microns | 3.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55576R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Uncured Silicone Rubber Interleave: LDPE This data represents typical values for the production material. T.. |
|||
Thickness | 76.2 microns | 3.00 mil | Interleave 1 |
Arlon 55581R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: 162 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum on.. |
|||
Thickness | 76.2 microns | 3.00 mil | Polyethylene , Interleave |
Arlon 75400R045 0.045" (1.14 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info.. |
|||
Thickness | 76.2 microns | 3.00 mil | Interleave |
Arlon LW401B##-P2 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Thickness | 76.2 microns | 3.00 mil | Carrier |
Arlon Thermabond® 99720W015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction:Liner: 0.001" FEP FilmSide 1: Uncured Silicone RubberCarrier: 0.003" PTFE coated FiberglassRecommended Primer: Dow Corning S2260This data represents typical values for the pr.. |
|||
Thickness | 76.2 microns | 3.00 mil | Carrier |
Arlon Thermabond® 99730N004 0.004" (0.102 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Electrically Conductive - Thermabond®. Bonds with primer.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Coring.. |
|||
Thickness | 76.2 microns | 3.00 mil | Carrier |
Arlon Thermabond® T20 (99710W008) 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: 8 mil thick Thermabond® T20 electrically insulating electronic adhesive.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Prim.. |
|||
Thickness | 76.2 microns | 3.00 mil | Facestock |
3M FM292 Indoor UL Recognized Clear Polyester Overlaminate Label Products 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 8000-114 Graphic Film This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 8000LF-12 Graphic Film This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ RG3650-114 Graphic Film 2-mil, opaque white and transparent film; Pressure-sensitive adhesive; Permanent filmInformation provided by 3M |
|||
Thickness | 76.2 microns | 3.00 mil | Interleave |
Arlon 32580R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. .. |
|||
Thickness | 76.2 microns | 3.00 mil | Liner |
3M 401M Double Coated Paper Tapes 3M™ Double Coated Paper Tapes 401M and 410M utilize a natural rubber adhesive system that offers good to excellent adhesion to many types of surfacesInformation provided by 3M |
|||
Thickness | 76.2 microns | 3.00 mil | Release Liner |
3M 4052 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Thickness | 76.2 microns | 3.00 mil | Interleave 2 |
Arlon 51576R015D 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical v.. |
|||
Thickness | 76.2 microns | 3.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51581B015 0.015" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: 2.5 mil LDPESide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: 2.5 mil LDPEThis data represents typical.. |
|||
Thickness | >= 76.2 microns | >= 3.00 mil | Side 1 |
Arlon 51586B015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Black silicone gum and rubber on fiberglass clothThis data Represents typical values for the production m.. |
|||
Thickness | 76.2 microns | 3.00 mil | Interleave |
Arlon 55560R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for.. |
|||
Thickness | 76.2 microns | 3.00 mil | Polyethylene, Interleave |
Arlon R31551R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Thickness | 76.2 microns | 3.00 mil | Polyethylene, Interleave |
Arlon R31678R016 0.0175" (0.444 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone/Kapton Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass cloth with Kapton® film on opposite side.This data Represents typical va.. |
|||
Thickness | 76.2 microns | 3.00 mil | Liner |
3M FM046 Clear Polyester Label Product 3M™ Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for demanding applications such.. |
|||
Thickness | 76.2 microns | 3.00 mil | Interleave |
Arlon 31560R015 0.015" (0.381 mm) Uncured Silicone Rubber on Release Carrier Design/Construction: Interleave: PolyethyleneProduct: Uncured Silicone Rubber Release Carrier: HDPE Carrier This data represents typical values for the production material. The data should not be us.. |
|||
Thickness | 76.2 microns | 3.00 mil | ASTM D3652 |
3M 3112 (Clear) Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 3112 has a low-tack adhesive system to help provide temporary protection in general industrial applications for many polished metals, plastics, glass materials and.. |