Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 50.8 microns | 2.00 mil | |
Rogers Corporation XT/duroid™ 8000 Thermoplastic Laminate, Circuit Material XT/duroid™ 8000 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. XT/duroid 8000 circuit materials ar.. |
|||
Thickness | 50.8 microns | 2.00 mil | Backing |
Dielectric Polymers NT-9512 Powder Coating Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Fine line definitionClean tape removalGood conformabilityNo film shrinkage after exposure to elevated temperaturesAbrasion resista.. |
|||
Thickness | 50.8 microns | 2.00 mil | |
Dow DOWLEX™ 2077G Linear Low Density Polyethylene Fast processing on narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Thickness | 50.8 microns | 2.00 mil | |
Dow INTEGRAL™ 917 Monolayer Bonding Film INTEGRAL 917 Adhesive Film is a single layer adhesive film for use where a higher flow rate and lower melt point are required. It is useful for bonding heat sensitive materials, or for porous subst.. |
|||
Thickness | 50.8 microns | 2.00 mil | Adhesive |
3M 9471 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Thickness | 50.8 microns | 2.00 mil | Tape |
3M 9497 Splicing Tapes 3M™ Splicing Tapes utilize on acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M |
|||
Thickness | 50.8 microns | 2.00 mil | Facestock |
3M FM045 Clear Polyester Label Product 3M™ Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for demanding applications such.. |
|||
Thickness | 50.8 microns | 2.00 mil | Facestock |
3M FM099 Indoor UL Recognized Matte Silver Polyester Label Product 3M™ Indoor UL Recognized Matte Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Thickness | 50.8 microns | 2.00 mil | Facestock |
3M FM1183 Indoor UL Recognized MC Polyester Label Products 3M™ Indoor UL Recognized MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These po.. |
|||
Thickness | 50.8 microns | 2.00 mil | Facestock |
3M FM123 Indoor UL Recognized White Polyester Label Products 3M™ Indoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ A.. |
|||
Thickness | 50.8 microns | 2.00 mil | Facestock |
3M FM157P Indoor UL Recognized Computer Imprintable Silver Polyester Label Product 3M™ Indoor UL Recognized Computer Imprintable Silver Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products a.. |
|||
Thickness | 50.8 microns | 2.00 mil | Liner |
3M FM157P Indoor UL Recognized Computer Imprintable Silver Polyester Label Product 3M™ Indoor UL Recognized Computer Imprintable Silver Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products a.. |
|||
Thickness | 50.8 microns | 2.00 mil | Facestock |
3M FP021 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Thickness | 50.8 microns | 2.00 mil | without adhesive |
3M Scotchcal™ 1000-89 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Thickness | 50.8 microns | 2.00 mil | without adhesive |
3M Scotchcal™ 3650-10 Graphic Film 2-mil opaque film; Available in white, black and transparent; Pressure-sensitive adhesive; Resists gasoline vapors and occasional petroleum spills; Permanent filmInformation provided by 3M |
|||
Thickness | 50.8 microns | 2.00 mil | without adhesive |
3M Scotchcal™ ElectroCut™ 7725-66 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 50.8 microns | 2.00 mil | Backing; ASTM D3752 |
3M 5480 PTFE Skived Film Tape 3M™ PTFE Skived Film Tape 5480 is a film backing with a silicone adhesive.Information provided by 3M |
|||
Thickness | 50.8 microns | 2.00 mil | Facestock |
3M 7237 HP Indigo Optimized Polyester Label Product 3M™ HP Indigo Optimized Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1400, which is a high performance tackified acry.. |
|||
Thickness | 50.8 microns | 2.00 mil | Adhesive |
3M 7957MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Thickness | >= 50.8 microns | >= 2.00 mil | Side 1, Rubber |
Arlon R31678R016 0.0175" (0.444 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone/Kapton Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass cloth with Kapton® film on opposite side.This data Represents typical va.. |
|||
Thickness | 50.8 microns | 2.00 mil | Facestock |
3M FM095 Indoor UL Recognized Matte Silver Polyester Label Product 3M™ Indoor UL Recognized Matte Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Thickness | 50.8 microns | 2.00 mil | Facestock |
3M FM167 Indoor UL Recognized Computer Imprintable White Polyester Label Product 3M™ Indoor UL Recognized Computer Imprintable White Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar.. |
|||
Thickness | 50.8 microns | 2.00 mil | without adhesive |
3M Scotchcal™ ElectroCut™ 7725-130 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 50.8 microns | 2.00 mil | without adhesive |
3M Scotchcal™ ElectroCut™ 7725-263 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 50.8 microns | 2.00 mil | without adhesive |
3M Scotchcal™ ElectroCut™ 7725-53 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 50.8 microns | 2.00 mil | Backing; ASTM D3752 |
3M 8992 Polyester Tape 3M™ Polyester Tape 8992 is a dark green polyester tape with silicone adhesive. It can be used in a large variety of high temperature applications including powdercoat masking, flashbreaker, and bag.. |
|||
Thickness | 50.8 microns | 2.00 mil | Facestock |
3M FM01961K MC Polyester Label Product 3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz.. |
|||
Thickness | 50.8 microns | 2.00 mil | Facestock |
3M FM023 Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |