Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 483 microns | 19.0 mil | |
Polystrand ThermoPro™ IE7020X X-Ply Cross-Ply Polyethylene-Glass Composite 2-Ply with Fiber Orientation at 0° & 90°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary ther.. |
|||
Thickness | 483 microns | 19.0 mil | per ply, 8HS form |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, C2 Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
Thickness | 483 microns | 19.0 mil | |
Hexcel® HexForce™ 384 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Thickness | 483 microns | 19.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 51588R019 0.019" (0.483 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2, Layer 1: Cured Silicone RubberSide 2, Layer 2: Uncured Silicone Rubber Interleave: Polyethylene Appearanc.. |
|||
Thickness | 483 microns | 19.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55572AA024 0.024" (0.610 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass This data represents typical values for the production material. The data should not be us.. |
|||
Thickness | 483 microns | 19.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55578R030 0.0325" (0.825 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1, Layer 2: Uncured Silicone Rubber Side 1, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Cured Silicone Rubber Appearance:.. |
|||
Thickness | 483 microns | 19.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55578XA030 0.032" (0.813 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: 162 Style Fiberglass Side 1: Cured Silicone Rubber (Skim Coat).. |
|||
Thickness | 483 microns | 19.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55586XC028 0.0295" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Thickness | 483 microns | 19.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55866R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material .. |
|||
Thickness | 483 microns | 19.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55869R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia.. |
|||
Thickness | 483 microns | 19.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55869R062 0.062" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia.. |
|||
Thickness | 483 microns | 19.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55989R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia.. |
|||
Thickness | 483 microns | 19.0 mil | Prime Coated 7500 Fiberglass, Substrate |
Arlon R35121R063 0.063" (1.60 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material speci.. |
|||
Thickness | 483 microns | 19.0 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51946C030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 1: Cured Silicone Wash Coat Appearance: Brown silicone rubber and gum on fiberglass.. |
|||
Thickness | 483 microns | 19.0 mil | substrate; Arlon SQA-TMS-003 |
Arlon 55096R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 2523 fiberglass; Side 2: uncured silicone rubber |
|||
Thickness | 483 microns | 19.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55102R024 0.024" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production material and should not be used as material specifications.In.. |
|||
Thickness | 483 microns | 19.0 mil | substrate; Arlon SQA-TMS-003 |
Arlon 55106R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber |
|||
Thickness | 483 microns | 19.0 mil | substrate; Arlon SQA-TMS-003 |
Arlon 55109R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: cured silicone rubber; Substrate: 162 fiberglass |
|||
Thickness | 483 microns | 19.0 mil | substrate; Arlon SQA-TMS-003 |
Arlon 55146R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber |
|||
Thickness | 483 microns | 19.0 mil | Style 162 Fiberglass, Substrate; Arlon SQA-TMS-003 |
Arlon 55146XA028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber This data represents typical values for the production mat.. |
|||
Thickness | 483 microns | 19.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55149R028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red si.. |
|||
Thickness | 483 microns | 19.0 mil | substrate; Arlon SQA-TMS-003 |
Arlon 55149R062 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: cured silicone rubber; Substrate: 162 fiberglass |
|||
Thickness | 483 microns | 19.0 mil | |
Aremco Pyro-Tape™ 682-PM High Temperature Tape Tri-layer silicone rubber/aluminum foil/ fiberglass with silicone adhesive Applications Plasma Spray Masking Features Multi-ply construction replaces single-ply tapes permitting significant reduction in masking time. Shadow mask tape for HVOF (high velocity oxy- fuel) spr.. |
|||
Thickness | 483 microns | 19.0 mil | substrate; Arlon SQA-TMS-003 |
Arlon 55279R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: cured silicone rubber; Substrate: 162 fiberglass |
|||
Thickness | 483 microns | 19.0 mil | |
Polystrand ThermoPro™ IE7021X ECR X-Ply Cross-Ply Polyethylene-Glass Composite 2-Ply with Fiber Orientation at 0° & 90°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary ther.. |
|||
Thickness | 483 microns | 19.0 mil | substrate; Arlon SQA-TMS-003 |
Arlon 55276R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber |