Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 15.0 - 50.0 microns | 0.591 - 1.97 mil | Recommended |
Polimeri Europa Flexirene® FF 25 Butene Copolymer Linear Low Density Polyethylene Flexirene FF 25 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FF 25 is characterized by a high elongational viscosi.. |
|||
Thickness | 15.0 - 50.0 microns | 0.591 - 1.97 mil | Recommended |
Polimeri Europa Flexirene® FG 20 U Butene Copolymer Linear Low Density Polyethylene Flexirene FG 20 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 U is recommended for the .. |
|||
Thickness | 15.0 - 50.0 microns | 0.591 - 1.97 mil | Recommended |
Polimeri Europa Flexirene® FG 23 I Butene Copolymer Linear Low Density Polyethylene Flexirene FG 23 I is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FG 23 I represents the version of Flexirene FG 20 I.. |
|||
Thickness | 15.0 - 50.0 microns | 0.591 - 1.97 mil | Recommended |
Polimeri Europa Flexirene® FG 23 U Butene Copolymer Linear Low Density Polyethylene Flexirene FG 23 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FG 23 U represents the version of Flexirene FG 20 U.. |
|||
Thickness | 15.0 - 50.0 microns | 0.591 - 1.97 mil | Recommended |
Polimeri Europa Flexirene® FH 56 A Butene Copolymer Linear Low Density Polyethylene Flexirene FH 56 A is a butene copolymer with medium density (C4-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Flexirene FH 56 A are characte.. |
|||
Thickness | 15.0 microns | 0.591 mil | |
SABIC F00952 High Density Polyethylene for Blown Film Product Description: F00952 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Thickness | 15.0 microns | 0.591 mil | |
SABIC F00952EQ High Density Polyethylene for Blown Film Product Description: F00952EQ is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. the design of the product, molecular architect.. |
|||
Thickness | 15.0 microns | 0.591 mil | |
SABIC F01552 High Density Polyethylene for Blown Film Product Description: F01552 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Thickness | 15.0 microns | 0.591 mil | |
SABIC FJ00952 High Density Polyethylene for Blown Film Product Description: FJ00952 is a TNPP additive free, high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, .. |
|||
Thickness | 15.0 - 50.0 microns | 0.591 - 1.97 mil | Recommended |
Polimeri Europa Flexirene® FG 20 I Butene Copolymer Linear Low Density Polyethylene Flexirene FG 20 I is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 I is recommended for the .. |
|||
Thickness | 15.0 - 50.0 microns | 0.591 - 1.97 mil | Recommended |
Polimeri Europa Flexirene® FG 23 F Butene Copolymer Linear Low Density Polyethylene Flexirene FG 23 F is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FG 23 F represents the version of Flexirene FG 20 F.. |
|||
Thickness | 15.0 microns | 0.591 mil | ± 3.5%; ASTM-252-78 |
Kinlead ML11 General Grade BOPP Matt Film (thickness: 15 µm) ML11 is a general grade BOPP Matt film. It is translucent and non heat sealable. It has low static and a good matt surface. One side has corona treatment. It is specially designed for board laminati.. |
|||
Thickness | 15.0 microns | 0.591 mil | ± 3.5%; ASTM-252-78 |
Kinlead ML21 General Grade BOPP Matt Film (thickness: 15 µm) ML21 is a general grade BOPP Matt film. It is translucent and non heat sealable. It has low static and a good matt surface. Both sides have corona treatment. It is specially designed for board lamin.. |
|||
Thickness | 15.0 microns | 0.591 mil | ± 3.5%; ASTM-252-78 |
Kinlead PL11 Lamination Grade BOPP Plain Film (thickness: 15 µm) PL11 is a general, lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. One side has corona treatment. It is widely used in laminating.. |
|||
Thickness | 15.0 microns | 0.591 mil | ± 3.5%; ASTM-252-78 |
Kinlead PL13 Lamination Grade BOPP Plain Film (thickness: 15 µm) PL13 is a woven bag lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. One side has corona treatment. It is widely used in laminatin.. |
|||
Thickness | 15.0 microns | 0.591 mil | ± 3.5%; ASTM-252-78 |
Kinlead PL21 Lamination Grade BOPP Plain Film (thickness: 15 µm) PL21 is a general, lamination grade BOPP plain film. It is transparent and non heat sealable. It is excellent for extrusion lamination. It has excellent dimensional stability, high tensile strength,.. |
|||
Thickness | 15.0 microns | 0.591 mil | ± 3.5%; ASTM-252-78 |
Kinlead PM11 Metalizing Grade BOPP Plain Film (thickness: 15 µm) PM11 is a general, metalizing grade BOPP plain film. It is transparent and non heat sealable. It has good heat resistance and tensile strength, and it has excellent metal adhesion. One side has coro.. |
|||
Thickness | 15.0 - 30.0 microns | 0.591 - 1.18 mil | |
Möller Medical NanoSkin 78 NanoCoating Transparent, scratch-resistant coating also for plastics with good resistance against dissolvents.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Thickness | 15.0 - 40.0 microns | 0.591 - 1.57 mil | |
Möller Medical PolySkin 80 NanoCoating Flexible, non-abrasive, decorative coating hardening at room temperature up to 120°C.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Thickness | 15.0 - 30.0 microns | 0.591 - 1.18 mil | |
Möller Medical PolySkin 81 NanoCoating Flexible, non-abrasive, decorative coating; easy-to-clean effect can be addedInformation provided by Möller Medical, Member of CENTROTEC Group |
|||
Thickness | 15.0 - 40.0 microns | 0.591 - 1.57 mil | |
Möller Medical PolySkin 82 NanoCoating Flexible, very non-abrasive, chemical-resistant decorative coating.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Thickness | 15.0 - 40.0 microns | 0.591 - 1.57 mil | |
Möller Medical PolySkin 95 NanoCoating Flexible, very non-abrasive, chemical-resistant decorative coating with easy-to-clean propertiesInformation provided by Möller Medical, Member of CENTROTEC Group |
|||
Thickness | 15.0 - 40.0 microns | 0.591 - 1.57 mil | |
Möller Medical TafSkin 98 NanoCoating Flexible, non-abrasive, temperature-stable, dirt-repellant coating, biocompatibleInformation provided by Möller Medical, Member of CENTROTEC Group |
|||
Thickness | 15.0 microns | 0.591 mil | |
SIDPEC EGYPTENE® HD 3802 FA HDPE Film Applications:General purpose thin film, trash bags, merchant bagsBlending partnerFilm properties were measured on 15 micron film extruded at a blow up ratio of 5:1, 10D neck height.Information provi.. |
|||
Thickness | 15.0 microns | 0.591 mil | |
SIDPEC EGYPTENE® HD 4602 FA HDPE Film Applications:Strong filmTrash bagShopping bagFilm properties were measured on 15 micron film extruded at a blow up ratio of 5:1, 8D neck height.Information provided by Interchim s.r.l., official dis.. |
|||
Thickness | 15.0 microns | 0.591 mil | |
SIDPEC EGYPTENE® HD 5301 FB HDPE Film Applications:Strong thin filmCarrier bagGrocery sacksFilm properties were measured on 15 micron film extruded at a blow up ratio of 5:1, 8D neck height.Information provided by Interchim s.r.l., offi.. |
|||
Thickness | 15.0 microns | 0.591 mil | |
SIDPEC EGYPTENE® LL 0209 AA LLDPE Film Applications:Heavy duty sacksAgricultural films and linersProduce bags, stretch filmFilm properties were measured on 15 micron film extruded at a blow up ratio of 2:1.Information provided by Interch.. |
|||
Thickness | 15.0 microns | 0.591 mil | As Tested |
Equate EGDA-6888 HDPE Film Extrusion Resin EGDA-6888 is a high molecular weight, high density polyethylene copolymer that has been designed specifically for tubular film extrusion. Its broad molecular weight distribution and density have bee.. |
|||
Thickness | 15.0 - 30.0 microns | 0.591 - 1.18 mil | |
Dow CYCLOTENE™ XU35075 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB) CYCLOTENE™ XU35075 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf.. |
|||
Thickness | 15.0 - 40.0 microns | 0.591 - 1.57 mil | |
Möller Medical NanoSkin Magic 112 NanoCoating Thermal resistant coating with outstanding easy-to-clean effect and chemical resistance, bioinertInformation provided by Möller Medical, Member of CENTROTEC Group |