Physical Properties Metric English Comments
Thickness 7.00 - 10.0 microns
0.276 - 0.394 mil
Fired
Lord Adhesives Metech 3614 Gold Conductor
Gold conductor composition 3614 is a thin print, mixed bond conductor. It has been formulated for both inner layer use in multilayer hybrids as well as for smooth, flat wire bond pads to optimize yi..
Thickness 7.00 microns
0.276 mil
Filament Diameter
Toho Tenax Tenax® HTA 5131 Chopped Carbon Fiber
Sized for Epoxy. Used in epoxy, phenolic, PBT, polycarbonate, polyethylene, polypropylene, and PPS. Information provided by Toho Carbon Fibers, a wholly owned subsidiary of Toho Tenax Co., Ltd.
Thickness 7.00 microns
0.276 mil
Filament Diameter
Toho Tenax Tenax® HTA 5N51 Chopped Carbon Fiber
Sized for Polyamide. Used in polyamide (nylon), PBT, polyethylene, PEI, PETP, and PPS. Information provided by Toho Carbon Fibers, a wholly owned subsidiary of Toho Tenax Co., Ltd.
Thickness 7.00 microns
0.276 mil
Filament Diameter
Toho Tenax Tenax® HTA 5U41 Chopped Carbon Fiber
Sized for polyurethane. Used in polyurethane, polyamide (nylon) and POM (acetal). Information provided by Toho Carbon Fibers, a wholly owned subsidiary of Toho Tenax Co., Ltd.
Thickness 7.00 - 10.0 microns
0.276 - 0.394 mil
Eifeler Coatings Technology TiN/TiC CVD Coating
The titanium nitride / titanium carbide combination layer is a standard layer well-proven over a long time. It indicates the following properties: Very high hardness; Very good adhesion; Suffic..
Thickness 7.00 - 14.0 microns
0.276 - 0.551 mil
Dow CYCLOTENE™ 4026-46 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)