Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 12.7 - 140 microns | 0.500 - 5.50 mil | Average value: 63.0 microns Grade Count:24 |
Overview of materials for Cyanoacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Thickness | 63.5 - 140 microns | 2.50 - 5.50 mil | Side 1 |
Arlon 19566R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The.. |
|||
Thickness | 63.5 - 140 microns | 2.50 - 5.50 mil | Side 1 |
Arlon 19576R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mat.. |
|||
Thickness | 63.5 - 140 microns | 2.50 - 5.50 mil | Side 1 |
Arlon R34896R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Thickness | 100 - 140 microns | 3.94 - 5.51 mil | |
P & P Technology NF32B050A21 Nylon/PET/Cu+Ni Conductive Fabric P & P Technology material reference NF32B050A21 is a metalised conductive fabric designed for use in EMC shielding and in the manufacture of conductive EMC gaskets. The material is a rip-stop weave .. |