Polymer Property : Thickness = 14.0 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 10.0 - 14.0 microns
0.394 - 0.551 mil
Fired
Lord Adhesives Metech 3288 Silver Conductor
This product is a silver paste composition designed for screen print application of a solderable electrode base onto various types of electrical ceramic component devices. The fired film forms a hig..
Thickness 12.0 - 14.0 microns
0.472 - 0.551 mil
Fired
Lord Adhesives Metech 3541 Platinum Silver Conductor Composition
These conductor compositions employ a state of the art mixed bond frit system to enhance adhesion and conductivity values while offering a range of cost effective conductors compatible with most res..
Thickness 12.0 - 14.0 microns
0.472 - 0.551 mil
Fired
Lord Adhesives Metech 3542 Platinum Silver Conductor Composition
These conductor compositions employ a state of the art mixed bond frit system to enhance adhesion and conductivity values while offering a range of cost effective conductors compatible with most res..
Thickness 12.0 - 14.0 microns
0.472 - 0.551 mil
Fired
Lord Adhesives Metech 3543 Platinum Silver Conductor Composition
These conductor compositions employ a state of the art mixed bond frit system to enhance adhesion and conductivity values while offering a range of cost effective conductors compatible with most res..
Thickness 12.0 - 14.0 microns
0.472 - 0.551 mil
Fired
Lord Adhesives Metech 3540 Platinum Silver Conductor Composition
These conductor compositions employ a state of the art mixed bond frit system to enhance adhesion and conductivity values while offering a range of cost effective conductors compatible with most res..
Thickness 7.00 - 14.0 microns
0.276 - 0.551 mil
Dow CYCLOTENE™ 4026-46 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
CYCLOTENE™ 4026-46 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf..