Polymer Property : Thickness = 800 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 800 microns
31.5 mil
Thickness tested
Thermoseal RG-N100 PTG Gasketing
Thermoseal RG-N100 is a nitrile butadiene rubber, reinforced cellulose fiber and mineral filler general purpose gasket material. Continuous roll lengths allow efficient and economical fabrication wi..
Thickness 800 microns
31.5 mil
Thickness tested
Thermoseal RG-N120 PTG Gasketing
Thermoseal RG-N120 is a reinforced cellulose gasket material with a nitrile butadiene rubber binder and inorganic fillers that provides a very good crush resistance at high flange pressures. Continu..
Thickness 800 microns
31.5 mil
Thickness tested
Thermoseal RG-P160 PTG Gasketing
Thermoseal RG-P160 is a blended fiber and polychloroprene rubber gasket material with mineral fillers. A factory applied release coating on both sides aid in flange removal. Continuous roll lengths ..
Thickness 800 microns
31.5 mil
Thickness tested
Thermoseal RG-S140 PTG Gasketing
Thermoseal RG-S140 is a controlled-swell gasket material that provides excellent sealing w here initial gasket conformability is required to compensate for flange out of flatness or roughness. After..
Thickness 800 microns
31.5 mil
Thickness tested
Thermoseal RG-S160 PTG Gasketing
Thermoseal RG-S160 offers exceptional sealability and crush resistance in a wide range of applications. RG-S160 is composed of a blend of aramid, mineral, and cellulose fibers and graphite and other..
Thickness 800 microns
31.5 mil
Overall; Arlon SQA-TMS-003
Arlon 55579R031H 0.0315" (0.800 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: LDPELayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. T..
Thickness 800 - 1590 microns
31.5 - 62.5 mil
Average value: 1330 microns Grade Count:3
Overview of materials for Chlorosulfonated Polyethylene Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Chlorosulfonated Polyethylene Rubber". Each property range of values reported is minimum and maximum val..