Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 7.00 - 10.0 microns | 0.276 - 0.394 mil | Fired |
Lord Adhesives Metech 3614 Gold Conductor Gold conductor composition 3614 is a thin print, mixed bond conductor. It has been formulated for both inner layer use in multilayer hybrids as well as for smooth, flat wire bond pads to optimize yi.. |
|||
Thickness | 7.00 microns | 0.276 mil | Filament Diameter |
Toho Tenax Tenax® HTA 5131 Chopped Carbon Fiber Sized for Epoxy. Used in epoxy, phenolic, PBT, polycarbonate, polyethylene, polypropylene, and PPS. Information provided by Toho Carbon Fibers, a wholly owned subsidiary of Toho Tenax Co., Ltd. |
|||
Thickness | 7.00 microns | 0.276 mil | Filament Diameter |
Toho Tenax Tenax® HTA 5N51 Chopped Carbon Fiber Sized for Polyamide. Used in polyamide (nylon), PBT, polyethylene, PEI, PETP, and PPS. Information provided by Toho Carbon Fibers, a wholly owned subsidiary of Toho Tenax Co., Ltd. |
|||
Thickness | 7.00 microns | 0.276 mil | Filament Diameter |
Toho Tenax Tenax® HTA 5U41 Chopped Carbon Fiber Sized for polyurethane. Used in polyurethane, polyamide (nylon) and POM (acetal). Information provided by Toho Carbon Fibers, a wholly owned subsidiary of Toho Tenax Co., Ltd. |
|||
Thickness | 7.00 - 10.0 microns | 0.276 - 0.394 mil | |
Eifeler Coatings Technology TiN/TiC CVD Coating The titanium nitride / titanium carbide combination layer is a standard layer well-proven over a long time. It indicates the following properties: Very high hardness; Very good adhesion; Suffic.. |
|||
Thickness | 7.00 - 14.0 microns | 0.276 - 0.551 mil | |
Dow CYCLOTENE™ 4026-46 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB) CYCLOTENE™ 4026-46 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf.. |