Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 508 - 1500 microns | 20.0 - 59.0 mil | Range of Thicknesses Available |
Rogers Corporation Poron® 4790-92-12 P Series Urethane Foam, Extra Soft, Slow Rebound, PET Film Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Thickness | 508 microns | 20.0 mil | |
Polystrand ThermoPro™ IE7010X X-Ply Cross-Ply Polypropylene-Glass Composite 2-Ply with Fiber Orientation at 0° & 90°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary ther.. |
|||
Thickness | 508 microns | 20.0 mil | overall; Arlon SQA-TMS-003 |
Arlon A3020-B004-12 Silicone Rubber/Fiberglass Laminate
(discontinued **) Side 1: cured fusible silicone rubber; Substrate: 25% sinusoidal fiberglass; Side 2: cured fusible silicone rubber; Interleave: 1 mil PE film |
|||
Thickness | 508 microns | 20.0 mil | overall; Arlon SQA-TMS-003 |
Arlon A3020-T002-12 Silicone Rubber/Fiberglass Laminate
(discontinued **) Side 1: cured fusible silicone rubber; Substrate: 25% sinusoidal fiberglass; Side 2: cured fusible silicone rubber; Interleave: 1 mil PE film |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 31580R020 0.020" (0.508 mm) Uncured Silicone Rubber on HDPE Carrier
(discontinued **) Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: High Density PolyethyleneAppearance: Red silicone gum on polymer linerThis data represents typical values for the.. |
|||
Thickness | 508 microns | 20.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon MT920-10#3.3-P1 0.020" (0.508 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Description:0.020” thick x 1.0” wide x 3.33 yards long, Rectangular cross-section, Silicone, Self-Fusing Tape.Design/Construction: Interleave: Polyethylene Rubber: Cured Self-Fusing Silicone Rubbe.. |
|||
Thickness | 508 microns | 20.0 mil | |
GrafTech eGRAF® HITHERM™ HT-1220 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Thickness | 508 microns | 20.0 mil | Nominal |
DuPont™ Nomex® 410 Paper, 20 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Thickness | 508 - 610 microns | 20.0 - 24.0 mil | Overall |
Arlon 30090R022 0.022" (0.559 mm) Uncured Unsupported Silicone Rubber on Kodacel Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Kodacel Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The d.. |
|||
Thickness | 508 microns | 20.0 mil | overall; Arlon SQA-TMS-003 |
Arlon 51146R020 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 508 microns | 20.0 mil | Overall Thickness |
Arlon 51580R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Thickness | 508 microns | 20.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 51866R020 0.020" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-012 |
Arlon 920-05C##FR-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 0.5” Wide Rectangular .0.5 inch wide, 20 mil thick, Black, Rectangular cross-section, Se.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 920-10C##FR-P0 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Brown, Rectangular cross-section, Self-fu.. |
|||
Thickness | 508 microns | 20.0 mil | Rubber; Arlon SQA-TMS-012 |
Arlon 920-10Hxx-P0 0.020" Self-Fusing Silicone Rubber Tape 1 inch wide, 20 mil thick, yellow, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.D.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 920-10R##-P2 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Red, Rectangular cross-section, Self-fusi.. |
|||
Thickness | 508 microns | 20.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon LW201B##-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 20 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Thickness | 508 microns | 20.0 mil | Rubber; Arlon SQA-TMS-003 |
Arlon LW201B##-P2 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 20 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Thickness | 508 microns | 20.0 mil | Overall thickness |
Arlon R32390B020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 1165 FiberglassAll ingredients of product are listed in 21 CFR 177.26000This data represe.. |
|||
Thickness | 508 microns | 20.0 mil | |
3M Scotchkote™ 80BG 536 Urethane Elastomer Scotchkote Urethane Elastomer 80BG 536 has been specifically developed as an elastomeric system with a high degree of flexibility for resurfacing rubber components. Product Features:Properties simil.. |
|||
Thickness | 508 microns | 20.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 32580X030 0.030" (0.762 mm) Uncured Unsupported Silicone Rubber on a PET Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on PET CarrierAppearance: Gray silicone gum on polymer linerThis data represents typical values for the production material. The data .. |
|||
Thickness | 508 microns | 20.0 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51271R037 0.037" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the produ.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 51273R020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave: Polyethylene This data represents typical values for the production materia.. |
|||
Thickness | >= 508 microns | >= 20.0 mil | Side 2 |
Arlon R31246R060 0.060" (1.52 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Rubber LayerSide 2: Uncured Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, mate.. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R35232B020 0.020" (0.508 mm) Fully Cured Silicone Rubber Description: Fully cured, unsupported, static dissipation siliconeDesign/Construction:Liner: Polyethylene Product: Fully Cured Silicone RubberAppearance: Black cured siliconeThis data represents typ.. |
|||
Thickness | 508 microns | 20.0 mil | Overall |
Arlon R35366X020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 1: Cured Silicone Rubber Appearance: Gray gum on glass fiber fabricThis data represe.. |
|||
Thickness | 508 microns | 20.0 mil | |
Daikin NEOFLON AF-2500 PFA Film NEOFLON PFA film is a high performance film made from tetrafluoroethylene and perfluoroalkyl vinyl ether (PFA).Information provided by Daikin Industries. |
|||
Thickness | 508 microns | 20.0 mil | Silicone |
Arlon 41580R020 0.020" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Thickness | 508 microns | 20.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R38726R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured SiliconeProduct Use: Flexible heater substrateAppearance: Red colored, high .. |
|||
Thickness | 508 microns | 20.0 mil | Silicone; Arlon SQA-TMS-003 |
Arlon 32570XA020 0.020" Uncured Silicone Rubber on Polyester Film Carrier Design/Construction:Interleave: 0.0025" PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as .. |