Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon MT920-10#3.3-P1 0.020" (0.508 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon MT920-10#3.3-P1 0.020" (0.508 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description:0.020” thick x 1.0” wide x 3.33 yards long, Rectangular cross-section, Silicone, Self-Fusing Tape.Design/Construction: Interleave: Polyethylene Rubber: Cured Self-Fusing Silicone Rubber Cross-Section: 1.0” Wide Triangular Meets US Military Specification A-A59163 (supersedes Mil-I-46852C) except for sampling level and packaging. The following tests are conducted on one roll from each lot of tape per A-A-59163: Thickness, Width, Bond Strength, Tensile Strength, Elongation, Dielectric Strength, and Water Absorption.Product Use: Multi-use tapeAppearance: Various colored silicone rubber tape on polymer liner.This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
Silicone Property; Arlon SQA-TMS-024
Water Absorption 1.7 %
1.7 %
Arlon SQA-TMS-016
Thickness 63.5 microns
2.50 mil
Polyethylene, Interleave
508 microns
20.0 mil
Rubber; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property; ASTM D2240
Tensile Strength 7.79 MPa
1130 psi
Silicone Property; ASTM D412
Elongation at Break 560 %
560 %
Silicone Property; ASTM D412
Peel Strength 0.543 kN/m
3.10 pli
Bond Strength; Arlon SQA-TMS-015
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 34.3 kV/mm
870 kV/in
ASTM D149
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Black
Blue
Green
Natural
Vibrant Red
Yellow
Copyright © lookpolymers.com All Rights Reserved