Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 50.0 - 250 microns | 1.97 - 9.84 mil | Recommended |
Polimeri Europa Riblene® FC 26 Low Density Polyethylene - Blown Film Extrusion Riblene FC 26 is a high molecular weight low density polyethylene (LDPE), with added antiblocking agent, suitable for blown film extrusion. Riblene FC 26 is characterized by a high melt strength le.. |
|||
Thickness | 50.0 microns | 1.97 mil | |
Premix Thermoplastics PREFLEX E50 Polyphenylene Ether (PPO/PPE) PREFLEX films combine outstanding dielectric properties, good heat stability, low water absorption and chemical resistance in a way not available before. Also rigid boards made of the same material .. |
|||
Thickness | 50.0 microns | 1.97 mil | |
Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4 and LDPE Blend The Trilene® TS 8057 product is a blend with a high ratio of linear low-density polyethylene - butene copolymer (LLDPE) with low-density polyethylene (LDPE) providing elevated processability and en.. |
|||
Thickness | 50.0 microns | 1.97 mil | |
Petroquimica Triunfo Trithene® TS 7001 LDPE - Heavy Duty Low Friction Film The Trithene TS 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and low coefficient of fricti.. |
|||
Thickness | 50.0 microns | 1.97 mil | |
Petroquimica Triunfo Trithene® TS 9022 MDPE - Overwrap Packaging The Trithene TS 9022 resin is a medium-density polyethylene (MDPE) with good optical properties, excellent stiffness and processability, that warrants the production of thin films with good appearan.. |
|||
Thickness | 50.0 microns | 1.97 mil | |
Petroquimica Triunfo Trithene® TX 7001 LDPE - High Molecular Weight The Trithene TX 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and environmental stress crac.. |
|||
Thickness | 50.0 microns | 1.97 mil | |
Petroquimica Triunfo Trithene® TX 7010 LDPE - Medium Duty Film The Trithene® TX 7010 resin is a low-density polyethylene (LDPE) with high molecular weight, excellent processability with very good mechanical properties. Besides these properties, the material is.. |
|||
Thickness | 50.0 - 200 microns | 1.97 - 7.87 mil | Recommended |
Polimeri Europa Greenflex® FD 20 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 20 is an ethylene vinyl acetate copolymer (EVA) suitable for blown film extrusion. Films produced with Greenflex FD 20 exhibit good optical properties, high impact resistance, tensile .. |
|||
Thickness | 50.0 - 200 microns | 1.97 - 7.87 mil | Recommended |
Polimeri Europa Greenflex® FD 53 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 53 is an ethylene vinyl acetate copolymer (EVA), containing antiblocking agent, for blown film extrusion. Films produced with Greenflex FD 53 exhibit good sealing properties, high flex.. |
|||
Thickness | 50.0 microns | 1.97 mil | |
SABIC HP0322N Low Density Polyethylene for Blown Film Product Description: HP0322N is a Low Density Polyethylene grade suitable for producing heavy duty films and contains no slip or antiblock additives. It yields outstanding toughness and optical pr.. |
|||
Thickness | 50.0 microns | 1.97 mil | |
Petroquimica Triunfo Trithene® TU 8091 LDPE - Agricultural Film Trithene TU 8091 is a low-density polyethylene (LDPE) with high molecular weight, with excellent mechanical properties and good processability. These qualities ensure the production of very wide fil.. |
|||
Thickness | 50.0 microns | 1.97 mil | |
Petroquimica Triunfo Trithene® TX 7003 LDPE - Heavy Duty and Industrial Film The Trithene® TX 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and environmental stress cracking resistance (ESCR). Additionally, this product.. |
|||
Thickness | 50.0 microns | 1.97 mil | |
Petroquimica Triunfo Tritheva® TN 2007 EVA Copolymer The Tritheva TN 2007 resin is an Ethylene-Vinyl Acetate copolymer (EVA), developed to meet the multi-layer packaging needs where are required high strength, with high toughness, and excellent optica.. |
|||
Thickness | 50.0 microns | 1.97 mil | |
Petroquimica Triunfo Tritheva® TN 8093 EVA Copolymer The Tritheva TN 8093 resin is a fractional MI copolymer of Ethylene-Vinyl Acetate (EVA), developed to meet the multi-layer and blending film applications where are required high strength, with high .. |
|||
Thickness | 50.0 microns | 1.97 mil | ± 2.5%; ASTM-252-78 |
Kinlead PG13 Bag Grade BOPP Plain Film (thickness: 50 µm) PG13 is a printing, bag grade BOPP plain film. It is transparent and non heat sealable. It has excellent flatness and good ink adhesion. One side has corona treatment. It is widely used in gift wrap.. |
|||
Thickness | 50.0 microns | 1.97 mil | |
Total PPR 6280 Random Copolymer Polypropylene, Cast Film Extrusion Grade Total Petrochemicals PPR 6280 is a random copolymer polypropylene with a melt flow index of 7 g/10 min suitable for the cast extrusion of films with outstanding optical properties and easy heat weld.. |
|||
Thickness | 50.0 microns | 1.97 mil | film |
DSM Akulon® F127 PA6 Low/Medium Viscosity, Film Extrusion |
|||
Thickness | 50.0 microns | 1.97 mil | film |
DSM Akulon® F130-C3 PA6 Monofilament Grade, Extrusion Grade, Medium Viscosity, Lubricated |
|||
Thickness | 50.0 microns | 1.97 mil | film |
DSM Akulon® F132 PA6 Film Extrusion, High Viscosity |
|||
Thickness | 50.0 microns | 1.97 mil | film |
DSM Akulon® F136 PA6 Very High Viscosity, Film Extrusion |
|||
Thickness | 50.0 microns | 1.97 mil | film |
DSM Akulon® F136-E2 PA6 Very High Viscosity, Lubricated, Nucleated, Film Extrusion |
|||
Thickness | 50.0 microns | 1.97 mil | film |
DSM Akulon® F234-C PA6 Film Extrusion, High Viscosity, Lubricated |
|||
Thickness | 50.0 microns | 1.97 mil | Film |
DSM Akulon® XP36-C1 PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Thickness | 50.0 microns | 1.97 mil | film |
DSM Akulon® F128 PA6 Film Extrusion, Medium Viscosity |
|||
Thickness | 50.0 - 200 microns | 1.97 - 7.87 mil | |
Bapolene® 105F Low Density Polyethylene Film Resin Description: Bapolene LD105F is an unmodified low density polyethylene which extrudes into a low gloss high impact film. It contains antiblock additives and no slip additives. This product meets th.. |
|||
Thickness | 50.0 microns | 1.97 mil | |
Carmel Olefins IPETHENE® 210 Low Density Polyethylene IPETHENE® 210 is a low density polyethylene extrusion grade, containing no additives. It exhibits a good balance between mechanical and optical properties. APPLICATIONS IPETHENE® 210 is mainly u.. |
|||
Thickness | 50.0 microns | 1.97 mil | Average value: 50.0 microns Grade Count:16 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Thickness | 50.0 microns | 1.97 mil | |
Victrex® APTIV® 1300-100G Polyetheretherketone (PEEK) Polymer Film DescriptionAPTIV® 1300 film is the black version of unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance .. |