Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 30.5 microns | 1.20 mil | |
ExxonMobil Escorene® LL-1042 LLDPE Packaging Film Resin, Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown clarity film resin. Films made from LL-1042 have very good tensile properties and toughness in addition to good clarity The good st.. |
|||
Thickness | 30.5 microns | 1.20 mil | |
ExxonMobil Escorene® LL-1108 LLDPE Film/Sandwich Bag Resin; 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin formulated with high slip, medium antiblock and processing aid for narrow die gap extrusion. Films made from LL-1108 have.. |
|||
Thickness | 30.5 microns | 1.20 mil | |
ExxonMobil Escorene® LL-1117 LLDPE Film/Sandwich Bag Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin. Films made from LL-1117 have very good tensile properties and toughness. This resin's good strength and drawability all.. |
|||
Thickness | 30.5 microns | 1.20 mil | |
ExxonMobil Escorene® LL-3113 LLDPE/Hexene Premium High Strength 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope.. |
|||
Thickness | 30.5 microns | 1.20 mil | Nominal; ExxonMobil Method |
ExxonMobil Bicor® 120 AB-X OPP Film Product Description: Bicor AB-X is a two-side coated, sealable OPP film designed for general use in many applications, including overwrap, horizontal and vertical packaging. This film is suitable as.. |
|||
Thickness | 30.5 microns | 1.20 mil | ExxonMobil Method |
ExxonMobil Bicor™ 120 XRG-2 OPP Film Product Description: Bicor 120 XRG-2 is a one-side sealable OPP film that can be used as the inside web of a lamination where exceptional seal performance is required. The high-energy surface is int.. |
|||
Thickness | 30.5 microns | 1.20 mil | ExxonMobil Method |
ExxonMobil Bicor™ 30MB400 OPP Film Product Description: A heat sealable coextruded biaxially oriented polypropylene film that can be used on a wide range of packaging machines. 30MB400 can be either used as mono material or in lamina.. |
|||
Thickness | 30.5 microns | 1.20 mil | ExxonMobil Method |
ExxonMobil Bicor™ 30MB666 OPP Film Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle East, .. |
|||
Thickness | 30.5 microns | 1.20 mil | ExxonMobil Method |
ExxonMobil Bicor™ 30MB668 OPP Film Product Description: A high speed transparent, biaxially oriented polypropylene film, coated one side very low temperature seal (VLTS) coating. VLTS coating provides excellent performances on high s.. |
|||
Thickness | 30.5 microns | 1.20 mil | ExxonMobil Method |
ExxonMobil Bicor™ 30MBR666 OPP Film Product Description: Bicor 30MBR is a biaxially oriented transparent polypropylene film coated with humidity resistant acrylic on both sides. This film is designed to wrap products with a high moist.. |
|||
Thickness | 30.5 microns | 1.20 mil | |
ExxonMobil Hicor® 30 HF 104 OHD Film One-side sealable, one-side treated, coextruded, oriented high density polyethylene film. It is ideal for use in HFFS and VFFS machines. It is designed to be used unsupported or in laminated applic.. |
|||
Thickness | 30.5 microns | 1.20 mil | ExxonMobil Method |
ExxonMobil Label-Lyte® 30 LLG-101 Clear OPP Film Product Description: A clear, one-side treated, biaxially oriented polypropylene film that is used in roll-fed labeling. This film can be laminated to itself (at other gauges of LLG-101) or applied .. |
|||
Thickness | 30.5 microns | 1.20 mil | Nominal; ExxonMobil Method |
ExxonMobil Bicor® 120 CSR-2 OPP Film Product Description: Bicor CSR-2 is a one-side treated OPP film designed for cold seal release, either unsupported or as the outer web of a lamination.Availability: Latin America, North America and .. |
|||
Thickness | 30.5 microns | 1.20 mil | Nominal; ExxonMobil Method |
ExxonMobil Bicor® 120 LTSC OPP Film Product Description: Bicor LTSC is a two-side coated OPP film which is designed for use in high-speed or demanding horizontal, fin seal, packaging applications. The low-temperature seal coating (LTS.. |
|||
Thickness | 30.5 microns | 1.20 mil | Nominal; ExxonMobil Method |
ExxonMobil Bicor® 120 SLP OPP Film Product Description: Bicor SLP is a one-side treated, non-heat sealable OPP film designed for use as the outside web of a lamination. The treated print surface is intended as the print and laminatin.. |
|||
Thickness | 30.5 microns | 1.20 mil | Backing; ASTM D3652 |
3M 5836 Clean-Walk Unframed Mat 3M™ Clean-Walk Unframed Mats 5830 Series are a multi-sheeted adhesive system that removes dirt and contaminates from shoe soles, wheels and other passing objects on contact. Comprised of a thin adh.. |
|||
Thickness | 30.5 microns | 1.20 mil | Facestock |
3M FP08R2 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Thickness | 30.5 microns | 1.20 mil | Facestock |
3M FP531 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Thickness | 30.5 microns | 1.20 mil | Facestock |
3M FP532 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Thickness | 30.5 microns | 1.20 mil | Backing; ASTM D3652 |
3M Scotch® 3721 Industrial Cold Temperature Box Sealing Tape Scotch® Box Sealing Tape 3721 is an industrial cold temperature packaging tape for use at refrigeration temperatures, or at room temperature with subsequent storage at low temperatures. This produc.. |
|||
Thickness | 30.5 microns | 1.20 mil | Backing; ASTM D3652 |
3M Scotch® 3779 Security Message Box Sealing Tape Scotch® Security Message Box Sealing Tape 3779 is an industrial packaging tape used for box sealing specifically where security of the carton contents is a concern. The printed design along with th.. |
|||
Thickness | 30.5 microns | 1.20 mil | Backing; ASTM D3652 |
3M Scotch® 640 Transparent Film Tape Scotch® 640 is a transparent film tape used for sealing, tabbing, splicing, various inner-pack applications and garment applications. This product has a conformable backing and a consistent pressur.. |
|||
Thickness | 30.5 microns | 1.20 mil | Backing; ASTM D3652 |
3M 5830 Clean-Walk Unframed Mat 3M™ Clean-Walk Unframed Mats 5830 Series are a multi-sheeted adhesive system that removes dirt and contaminates from shoe soles, wheels and other passing objects on contact. Comprised of a thin adh.. |
|||
Thickness | 30.5 microns | 1.20 mil | Adhesive |
3M 7847 Laser Markable Label Material 3M™ Laser Markable Label Material 7847 and 7848 are specialty film label materials where a laser can ablate the top layer of a dual-layer facestock to create an image. The same laser can also kiss .. |
|||
Thickness | 30.5 microns | 1.20 mil | Adhesive |
3M 8417 Polyester Film Tape 3M™ Polyester Film Tape 8417 is a self-wound (linerless) transparent polyester film coated with 3M™ Adhesive 100 High-temperature Acrylic. It is often used as an overlaminate in conjunction with 3.. |
|||
Thickness | 30.5 microns | 1.20 mil | Backing; ASTM D3652 |
3M Scotch® 3781 Industrial Continuous Taping System Tape Scotch® Taping System Tape 3781 is an industrial continuous packaging tape used for box sealing and specially designed for use with the 3M-Matic™ Continuous Taping System (CTS) stand. The Product .. |
|||
Thickness | 30.5 microns | 1.20 mil | |
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su.. |
|||
Thickness | 30.5 microns | 1.20 mil | |
ExxonMobil Escorene® LL-3201 LLDPE/Hexene Premium High Strength 1.2 mil Film, Stiff
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope.. |
|||
Thickness | 30.5 microns | 1.20 mil | ExxonMobil Method |
ExxonMobil Oppalyte™ 30 HM-3 OPP Film Product Description: A white opaque OPP film with a proprietary cavitated core. HM-3 is designed for cold seal applications and is used as a surface print, monoweb, or as the inside of lamination. I.. |
|||
Thickness | 30.5 microns | 1.20 mil | ExxonMobil Method |
ExxonMobil Oppalyte™ 30MD447 OPP Film Product Description: A coextruded super white opaque, modified higher density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for u.. |